Heat deflection temperature, 0.45 MPa: 217 °C

Quick Comparison

Tereftalato de polibutileno (PBT)

LNP™ THERMOCOMP™ Compound WF006XXP

Suministrada por:

Sabic

Polyamide 612 (PA612)

Zytel® 77G43L NC010

Tereftalato de polibutileno (PBT)

LNP™ ELCRIN™ WF006JiQ

Suministrada por:

Sabic

Tereftalato de polibutileno (PBT)

VALOX™ Resin 420HP

Tereftalato de polibutileno (PBT)

LNP™ THERMOCOMP™ Compound WX05502

Suministrada por:

Sabic

Tereftalato de polibutileno (PBT)

LNP™ ELCRIN™ WF006XiQ

Suministrada por:

Sabic

Polieterimida (PEI)

LNP™ STAT-KON™ Compound EE004

Suministrada por:

Sabic

Polyamide 612 (PA612)

Zytel® 77G43L BK031

Polietersulfona (PES)

LNP™ THERMOCOMP™ Compound JF006LXZ

Suministrada por:

Sabic

Polyamide 6 (PA6)

LNP™ THERMOCOMP™ Compound PF007S

Suministrada por:

Sabic

Polietersulfona (PES)

LNP™ THERMOCOMP™ Compound JF006LZZ

Suministrada por:

Sabic

Tereftalato de polibutileno (PBT)

LNP™ LUBRICOMP™ Compound WFI14

Suministrada por:

Sabic

Tereftalato de polibutileno (PBT)

LNP™ LUBRICOMP™ Compound WAL34I

Suministrada por:

Sabic