Heat deflection temperature, 0.45 MPa: 235 °C

Quick Comparison

Polietileno tereftalato (PET)

Rynite® 935 NC010

Polietileno tereftalato (PET)

Rynite® 415HP NC010

Polyamide 410 (PA410)

EcoPaXX® Q-DWX10

Suministrada por:

DSM Engineering Materials

Polyamide 66 (PA66)

Zytel® FR7025V0F NC010

Polyamide 410 (PA410)

EcoPaXX® Q-KXG10

Suministrada por:

DSM Engineering Materials

Polyamide 410 (PA410)

EcoPaXX® Q-HGM24

Suministrada por: