Heat deflection temperature, 1.80 MPa: 188 °C

Quick Comparison

Polieterimida (PEI)

ULTEM™ Resin HU1100 - Americas

Suministrada por:

Sabic

Polieterimida (PEI)

ULTEM™ Resin HU1100 - Asia

Suministrada por:

Sabic

Polieterimida (PEI)

ULTEM™ Resin HU1100 - Europe

Suministrada por:

Sabic

Polieterimida (PEI)

ULTEM™ Resin 1000E - Europe

Suministrada por:

Sabic

Polieterimida (PEI)

ULTEM™ Resin 1000EF - Europe

Suministrada por:

Sabic

Polieterimida (PEI)

ULTEM™ Resin 1000EF - Asia

Suministrada por:

Sabic

Polieterimida (PEI)

ULTEM™ Resin 1000EF - Americas

Suministrada por:

Sabic

Polieterimida (PEI)

ULTEM™ Resin HU1000E - Europe

Suministrada por:

Sabic

Polieterimida (PEI)

ULTEM™ Resin HU1000E - Asia

Suministrada por:

Sabic

Polieterimida (PEI)

ULTEM™ Resin HU1000E - Americas

Suministrada por:

Sabic

Polyamide 612 (PA612)

LNP™ THERMOCOMP™ Compound IF006 - Europe

Suministrada por:

Sabic

Polyamide 612 (PA612)

LNP™ THERMOCOMP™ Compound IF004 - Asia

Suministrada por:

Sabic

Polieterimida (PEI)

ULTEM™ Resin 9075 - Asia

Suministrada por:

Sabic

Polieterimida (PEI)

ULTEM™ Resin 9075 - Americas

Suministrada por:

Sabic