ULTEM™ Resin HU1100 - Americas

Want to keep this datasheet? Save it now in your required format

Description

Standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change; biocompatible (ISO 10993 or USP Class VI); food contact compliant; Steam, Gamma, EtO, and E-beam sterilizable.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.27 g/cm³

Show Supplier Material materials with Density of 1.27 g/cm³

ISO 1183

Moisture absorption

23.0 °C

0.7 %

Show Supplier Material materials with Moisture absorption of 0.7 %

ISO 62 | (23°C / 50% RH)

Relative density

23.0 °C

1.36 [-]

Show Supplier Material materials with Relative density of 1.36 [-]

ASTM D 792

Water absorption

23.0 °C

1.25 %

Show Supplier Material materials with Water absorption of 1.25 %

ISO 62-1 | (23°C/saturated)

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

3.2 GPa

Show Supplier Material materials with Elastic modulus of 3.2 GPa

ISO 527 | 1 mm/min

Elongation

23.0 °C

60 %

Show Supplier Material materials with Elongation of 60 %

ISO 527 | break, 5 mm/min

Flexural modulus

23.0 °C

3.3 GPa

Show Supplier Material materials with Flexural modulus of 3.3 GPa

ISO 178 | 2 mm/min

Flexural strength

23.0 °C

160 MPa

Show Supplier Material materials with Flexural strength of 160 MPa

ISO 178 | yield, 2 mm/min

Impact strength, Charpy notched

23.0 °C

4 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 4 kJ/m²

ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, 23°C

Impact strength, Izod notched

23.0 °C

6 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 6 kJ/m²

ISO 180/1A | notched 80*10*4, -30°C

Instrumented Impact, Total Energy

23.0 °C

38 J

Show Supplier Material materials with Instrumented Impact, Total Energy of 38 J

ASTM D 3763 | 23°C

Tensile strength

23.0 °C

85 MPa

Show Supplier Material materials with Tensile strength of 85 MPa

ISO 527 | break, 5 mm/min

Impact strength, Izod notched, ASTM

ASTM D 256

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

5.5E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 5.5E-5 1/K

ISO 11359-2 | -40°C to 40°C

Coefficient of thermal expansion, transverse

23.0 °C

5.5E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion, transverse of 5.5E-5 1/K

ISO 11359-2 | -40°C to 40°C

Heat deflection temperature, 1.80 MPa

188 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 188 °C

ISO 75/Af | Flatw 80*10*4 sp=64mm

Relative temperature index, electrical

170 °C

Show Supplier Material materials with Relative temperature index, electrical of 170 °C

UL 746B

Relative temperature index, mechanical impact

170 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 170 °C

UL 746B

Relative temperature index, mechanical strength

170 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 170 °C

UL 746B

Vicat softening temperature

211 °C

Show Supplier Material materials with Vicat softening temperature of 211 °C

ISO 306 | Rate B/50

Flammability

UL Recognized, 94-5VA Flame Class Rating: ≥3mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100044765- -

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

4 V

Show Supplier Material materials with Comparative tracking index of 4 V

UL 746A | (UL) {PLC}

High Amp Arc Ignition

23.0 °C

0.75 mm

Show Supplier Material materials with High Amp Arc Ignition of 0.75 mm

≥, UL 746A | PLC 4

High Volt Arc Track Rate

23.0 °C

2 PLC Code

Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code

UL 746A | (PLC)

Hot-Wire Ignition

23.0 °C

3 mm

Show Supplier Material materials with Hot-Wire Ignition of 3 mm

≥, UL 746A | PLC 1

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

8.8 g/10min

Show Supplier Material materials with Melt mass-flow rate of 8.8 g/10min

ASTM D 1238 | 337°C/6.6 kgf

Melt volume-flow rate

16 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 16 cm³/10min

ISO 1133 | MVR at 220°C/5.0 kg

Shrinkage

23.0 °C

0.5 %

Show Supplier Material materials with Shrinkage of 0.5 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Surgical Devices, Pharmaceutical Manufacturing, Medical Device, Medical Facility Infrastructure

Availability

Europe,Asia,Americas

Features

High Stiffness, Healthcare management of change, Steam, Gamma, EtO and E-beam sterilizable, Hydrolytic Stability, Chemical Resistance, Low Smoke and Toxicity, Good Mechanicals in Broad Temperature Range, Low Creep Sensitivity, Low Shrinkage, Good metal adhesion, Amorphous, High Strength, High Heat Resistance, Good dimensional stability, Flame Retardant, Steam Sterilizable, Gamma Sterilizable, E-beam Sterilizable, Food Contact Acceptable, Biocompatible

Processing methods

Nozzle Temperature: 345 to 400.0°C
Shot to Cylinder Size: 40 to 60.0%
Drying Time (Cumulative): 24hrs
Drying Temperature: 150°C
Vent Depth: 0.025 to 0.076mm
Maximum Moisture Content: 0.02%
Front - Zone 3 Temperature: 345 to 400.0°C
Melt Temperature: 350 to 400.0°C
Rear - Zone 1 Temperature: 330 to 400.0°C
Mold Temperature: 135 to 165.0°C
Middle - Zone 2 Temperature: 340 to 400.0°C
Back Pressure: 0.3 to 0.7MPa
Screw Speed: 40 to 70.0rpm
Drying Time: 4 to 6.0hrs

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.