Impact strength, Charpy notched, ASTM: 64 J/m

Quick Comparison

Polyvinylidenefluoride (PVDF)

Kynar® 705

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 370

Suministrada por:

Arkema: High Performance Polymers

Polyamide 66 (PA66)

PA66 CF30

Suministrada por:

Xiamen Keyuan Plastic Co., Ltd

Tereftalato de polibutileno (PBT)

PBT GF30 V0

Suministrada por:

Xiamen Keyuan Plastic Co., Ltd

Acrilonitrilo butadieno estireno (ABS)

ABS GF30

Suministrada por:

Xiamen Keyuan Plastic Co., Ltd