PA66 CF30

Alternative and trade names
PA66-CF30
Want to keep this datasheet? Save it now in your required format

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.36 g/cm³

Show Supplier Material materials with Density of 1.36 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

2.5 %

Show Supplier Material materials with Elongation of 2.5 %

ASTM D638

Flexural modulus

23.0 °C

12.8 GPa

Show Supplier Material materials with Flexural modulus of 12.8 GPa

ASTM D790

Flexural strength

23.0 °C

282 MPa

Show Supplier Material materials with Flexural strength of 282 MPa

ASTM D790

Impact strength, Charpy notched, ASTM

23.0 °C

64 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 64 J/m

ASTM D256

Tensile strength

23.0 °C

186 MPa

Show Supplier Material materials with Tensile strength of 186 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

252 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 252 °C

ASTM D648

Melting point

275 °C

Show Supplier Material materials with Melting point of 275 °C

ASTM D2117

Flammability

UL94 HB

Rheological Properties

PropertyTemperatureValue

Shrinkage

23.0 °C

0.3 %

Show Supplier Material materials with Shrinkage of 0.3 %

Technological properties

Property
Application areas

New energy vehicles, smart devices, low-carbon travel equipment, mine equipment, etc.

Fillers

30% Carbon Fiber