ABS GF30

Alternative and trade names
ABS-GF30
Want to keep this datasheet? Save it now in your required format

Description

Acrylonitrile Butadiene Styrene (ABS) reinforced with 30% glass fiber

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.24 g/cm³

Show Supplier Material materials with Density of 1.24 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

5.63 GPa

Show Supplier Material materials with Flexural modulus of 5.63 GPa

ASTM D790

Hardness, Shore D

23.0 °C

82 [-]

Show Supplier Material materials with Hardness, Shore D of 82 [-]

ASTM D785

Impact strength, Charpy notched, ASTM

23.0 °C

64 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 64 J/m

ASTM D256

Tensile strength

23.0 °C

78 MPa

Show Supplier Material materials with Tensile strength of 78 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature

103 °C

Show Supplier Material materials with Heat deflection temperature of 103 °C

ASTM D648

Vicat softening temperature

115 °C

Show Supplier Material materials with Vicat softening temperature of 115 °C

ASTM D15255

Technological properties

Property
Fillers

30% Glass Fiber