Impact strength, Charpy notched, ASTM: 75 J/m

Quick Comparison

Polyvinylidenefluoride (PVDF)

Kynar® 705

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 370

Suministrada por:

Arkema: High Performance Polymers

Polyamide 6 (PA6)

PA6 GF25 FR V0

Suministrada por:

Xiamen Keyuan Plastic Co., Ltd

Polioximetileno (POM)

POM GF40

Suministrada por:

Xiamen Keyuan Plastic Co., Ltd

Polyamide 66 (PA66)

PA66 + PTFE15+GF30

Suministrada por:

Xiamen Keyuan Plastic Co., Ltd