PA66 + PTFE15+GF30

Alternative and trade names
PA66-PTFE15+GF30
Want to keep this datasheet? Save it now in your required format

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.49 g/cm³

Show Supplier Material materials with Density of 1.49 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

8 GPa

Show Supplier Material materials with Flexural modulus of 8 GPa

ASTM D790

Flexural strength

23.0 °C

200 MPa

Show Supplier Material materials with Flexural strength of 200 MPa

ASTM D790

Impact strength, Charpy notched, ASTM

23.0 °C

75 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 75 J/m

ASTM D256

Tensile strength

23.0 °C

125 MPa

Show Supplier Material materials with Tensile strength of 125 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

245 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 245 °C

ASTM D648

Flammability

UL94 HB

Rheological Properties

PropertyTemperatureValue

Shrinkage

23.0 °C

0.4 - 0.8 %

Show Supplier Material materials with Shrinkage of 0.4 - 0.8 %

Technological properties

Property
Application areas

Wide machinery, instrumentation, auto parts, electronic and electrical, railways, home appliances, communications, textile machinery, sports and leisure products, tubing, fuel tanks and some precision engineering products.

Fillers

30% Glass Fiber and 15% PTFE