POM GF40

Alternative and trade names
POM-GF40
Want to keep this datasheet? Save it now in your required format

Description

Polyoxymethylene (POM), reinforced with 40% glass fiber, is a Homopolymerize HB

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.7 g/cm³

Show Supplier Material materials with Density of 1.7 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

3 %

Show Supplier Material materials with Elongation of 3 %

ASTM D638

Flexural modulus

23.0 °C

10.3 GPa

Show Supplier Material materials with Flexural modulus of 10.3 GPa

ASTM D790

Flexural strength

23.0 °C

159 MPa

Show Supplier Material materials with Flexural strength of 159 MPa

ASTM D790

Impact strength, Charpy notched, ASTM

23.0 °C

75 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 75 J/m

ASTM D256

Tensile strength

23.0 °C

117 MPa

Show Supplier Material materials with Tensile strength of 117 MPa

ASTM D638

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

3.8E-4 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 3.8E-4 1/K

Heat deflection temperature

166 °C

Show Supplier Material materials with Heat deflection temperature of 166 °C

ASTM D648

Electrical

PropertyTemperatureValueComment

Dielectric strength

23.0 °C

20 kV/mm

Show Supplier Material materials with Dielectric strength of 20 kV/mm

ASTM D147

Technological properties

Property
Fillers

40% Glass Fiber