Impact strength, Izod notched, ASTM: 144 J/m

Quick Comparison

Policarbonato (PC)

LEXAN™ Copolymer HPH4504H - Asia

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer HPH4504 - Europe

Suministrada por:

Sabic

Tereftalato de polibutileno (PBT)

LNP™ THERMOTUF™ Compound WF009N

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound DFL22

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound DFL22ER

Suministrada por:

Sabic

Éter de polifenileno (PPE)

NORYL™ Resin HNA033 - Europe

Suministrada por:

Sabic

Éter de polifenileno (PPE)

NORYL™ Resin HNA033 - Asia

Suministrada por:

Sabic

Éter de polifenileno (PPE)

NORYL™ Resin HNA033 - Americas

Suministrada por:

Sabic

Éter de polifenileno (PPE)

NORYL™ Resin HNA055 - Asia

Suministrada por:

Sabic

Éter de polifenileno (PPE)

NORYL™ Resin HNA055 - Americas

Suministrada por:

Sabic

Polyamide 6 (PA6)

LNP™ THERMOTUF™ Compound PF008IR

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ THERMOCOMP™ Compound DF006LXN

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF009H

Suministrada por:

Sabic