Impact strength, Izod notched, ASTM: 310 J/m

Quick Comparison

Mezcla de polímeros

XENOY™ Resin 1731

Policarbonato (PC)

LEXAN™ Resin EM3110

Poliuretano termoplástico (TPU)

TPU LGU602

Suministrada por:

Great Eastern Resins Industrial Co. Ltd.