TPU LGU602

Alternative and trade names
LGU602
Want to keep this datasheet? Save it now in your required format

Description

High rigidity, Heat resistance, Dimensional stability

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

1.7 g/cm³

Show Supplier Material materials with Density of 1.7 g/cm³

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

2 %

Show Supplier Material materials with Elongation of 2 %

Flexural modulus

23.0 °C

15.5 GPa

Show Supplier Material materials with Flexural modulus of 15.5 GPa

Flexural strength

23.0 °C

290 MPa

Show Supplier Material materials with Flexural strength of 290 MPa

Impact strength, Izod notched, ASTM

23.0 °C

310 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 310 J/m

ASTM D256

Tensile strength

23.0 °C

210 MPa

Show Supplier Material materials with Tensile strength of 210 MPa

Rheological Properties

PropertyTemperatureValue

Shrinkage

23.0 °C

0.05 - 0.2 %

Show Supplier Material materials with Shrinkage of 0.05 - 0.2 %

Technological properties

Property
Application areas

Mechanical Parts, Medical equipment, Sports Equipment