Acero inoxidable austenítico
Alloy 24 / 1.4565 Solution annealed and quenchedSuministrada por:
Hempel Special MetalsAcero inoxidable dúplex
Sandvik SAF 2707 HD™Suministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable austenítico
ASTM A276 Grade S20910 AnnealedAcero inoxidable austenítico
SEW 400 Grade X2CrNiMnMoNbN25-18-5-4 quenched (+Q)Acero inoxidable austenítico
EN 10095 Grade X25CrMnNiN25-9-7 solution annealed (+AT)Acero inoxidable austenítico
EN 10090 Grade X50CrMnNiNbN21-9 solution heat-treated and precipitation hardened (+AT+P)Acero inoxidable austenítico
EN 10090 Grade X53CrMnNiN21-9 solution heat-treated and precipitation hardened (+AT+P)Acero inoxidable austenítico
EN 10090 Grade X55CrMnNiN20-8 solution heat-treated and precipitation hardened (+AT+P)Acero inoxidable austenítico
ASTM A213 Grade XM-19 Heat-TreatedAcero inoxidable austenítico
ASTM A688 Grade TPXM-29 Solution-AnnealedAcero inoxidable austenítico
DIN 17480 Grade X50CrMnNiNbN21-9 solution heat-treated and precipitation hardened (+AT+P)Acero inoxidable austenítico
DIN 17480 Grade X53CrMnNiN21-9 solution heat-treated and precipitation hardened (+AT+P)Acero inoxidable austenítico
ASTM A193 Grade B8R Class 1C, Carbide solution treatedAcero inoxidable austenítico
ASTM A193 Grade B8R Class 1D, Carbide solution treatedAcero inoxidable austenítico
ASTM A193 Grade B8RA Class 1C, Carbide solution treated in the finished conditionAcero inoxidable austenítico
ASTM A213 Grade S34565 Heat-TreatedAcero inoxidable austenítico
ASTM A240 Grade XM-19 Heat-Treated