Molybdenum Steel
EN 10028-2 Grade 16Mo3 normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Medium Carbon Steel
ISO 683-1 Grade C45 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Medium Carbon Steel
ISO 683-1 Grade C45 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Acero bajo en carbono
DIN 17200 Grade C22 normalized or normalized formed (+N)Acero inoxidable austenítico
DIN 17440 Grade X5CrNi18-10 quenched (+Q)Nickel Chromium Iron Alloy
DIN 17744 Grade NiCr19NbMo precipitation hardened (+P)Acero inoxidable austenítico
DIN 17440 Grade X5CrNi18-10 solution heat-treated and quenchedAcero inoxidable austenítico
DIN 17440 Grade X5CrNiMo17-12-2 solution heat-treated and quenchedAcero inoxidable austenítico
DIN 17440 Grade X5CrNiMo17-12-2 quenched (+Q)Acero bajo en carbono
EN 10277-5 Grade C22 cold drawn or turned and quenched and temperedChromium Molybdenum Steel
DIN 17176 Grade 12CrMo19-5 soft annealed (+A)Acero inoxidable austenítico
EN 10028-7 Grade X5CrNi18-10 solution annealed (+AT)Acero bajo en carbono
DIN 17200 Grade C22 quenched and tempered (+QT)Acero bajo en carbono
EN 10083-1 Grade C22 quenched and tempered (+QT)Acero inoxidable austenítico
EN 10272 Grade X5CrNi18-10 solution annealed (+AT)Acero inoxidable austenítico
EN 10272 Grade X5CrNiMo17-12-2 solution annealed (+AT)Chromium Molybdenum Steel
DIN 17176 Grade 12CrMo19-5 quenched and tempered (+QT2)Chromium Molybdenum Steel
DIN 17176 Grade 12CrMo19-5 quenched and tempered (+QT1)Acero inoxidable austenítico
EN 10028-7 Grade X5CrNiMo17-12-2 solution annealed (+AT)Acero bajo en carbono
EN 10277-5 Grade C22 cold drawn