Acero bajo en carbono
EN 10028-3 Grade P275NH normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Acero bajo en carbono
EN 10120 Grade P310NB normalized or normalized formed (+N)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10025-4 Grade S420M thermomechanically rolledSuministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10025-4 Grade S420ML thermomechanically rolledSuministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
ISO 683-2 Grade 33MnCrB5-2 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Carbon Steel
ASTM A516 Grade 380 As-Rolled or Normalized and/or Stress RelievedSuministrada por:
1 proveedor Matmatch
Unclassified Carbon Steel
ASTM A516 Grade 450 As-Rolled or Normalized and/or Stress RelievedSuministrada por:
1 proveedor Matmatch
Acero bajo en carbono
DIN 17200 Grade C22 quenched and tempered (+QT)Acero bajo en carbono
EN 10297-1 Grade 36Mn4 quenched and tempered (+QT)Medium Carbon Steel
EN 10083-2 Grade C35E quenched and tempered (+QT)Medium Carbon Steel
EN 10083-1 Grade C45E quenched and tempered (+QT)Medium Carbon Steel
EN 10083-2 Grade C35E quenched and tempered (+QT)Medium Carbon Steel
EN 10277-5 Grade C35 cold drawn or turned and quenched and temperedMedium Carbon Steel
EN 10277-5 Grade C45 cold drawn or turned and quenched and temperedMedium Carbon Steel
EN 10277-5 Grade Ck35 cold drawn or turned and quenched and tempered