General
Property | Value | Comment |
---|---|---|
Density | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elastic modulus | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel | |||
Elongation | 19.1 % Show Material materials with Elongation of 19.1 % | Predicted Value, Transverse | |||
19.5 % Show Material materials with Elongation of 19.5 % | Predicted Value, A80 | ||||
19.9 % Show Material materials with Elongation of 19.9 % | Predicted Value, A80 Transverse | ||||
23 % Show Material materials with Elongation of 23 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate | A200 | |
24.9 % Show Material materials with Elongation of 24.9 % | Predicted Value | ||||
27 % Show Material materials with Elongation of 27 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate | A50 | |
Hardness, Brinell | 241 [-] Show Material materials with Hardness, Brinell of 241 [-] | Predicted Value, Transverse | |||
Poisson's ratio | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel | |||
Reduction of area | 42.7 % Show Material materials with Reduction of area of 42.7 % | Predicted Value | |||
43.0 % Show Material materials with Reduction of area of 43.0 % | Predicted Value, Transverse | ||||
Shear modulus | 79.4 GPa Show Material materials with Shear modulus of 79.4 GPa | Predicted Value | |||
Shear strength | 504.6 MPa Show Material materials with Shear strength of 504.6 MPa | Predicted Value | |||
Tensile strength | 380 - 515 MPa Show Material materials with Tensile strength of 380 - 515 MPa | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate | |
Yield strength | 205 MPa Show Material materials with Yield strength of 205 MPa | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate | RP02 |
261.6 MPa Show Material materials with Yield strength of 261.6 MPa | Predicted Value, RP05 | ||||
271.2 MPa Show Material materials with Yield strength of 271.2 MPa | Predicted Value, RP1 | ||||
318.8 MPa Show Material materials with Yield strength of 318.8 MPa | Predicted Value, RP1 Transverse | ||||
358.9 MPa Show Material materials with Yield strength of 358.9 MPa | Predicted Value, Transverse | ||||
393.8 MPa Show Material materials with Yield strength of 393.8 MPa | Predicted Value, RP02 Transverse | ||||
405.5 MPa Show Material materials with Yield strength of 405.5 MPa | Predicted Value, RP002 |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 11.83 1/K Show Material materials with Coefficient of thermal expansion of 11.83 1/K | Predicted Value |
Max service temperature | 309.6 °C Show Material materials with Max service temperature of 309.6 °C | Predicted Value, Long |
Specific heat capacity | 457.4 J/(kg·K) Show Material materials with Specific heat capacity of 457.4 J/(kg·K) | Predicted Value |
Thermal conductivity | 40.08 W/(m·K) Show Material materials with Thermal conductivity of 40.08 W/(m·K) | Predicted Value |
Electrical
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Carbon | 0.18 % Show Material materials with Carbon of 0.18 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate |
Manganese | 0.6 - 0.9 % Show Material materials with Manganese of 0.6 - 0.9 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate |
Phosphorus | 0.025 % Show Material materials with Phosphorus of 0.025 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate |
Silicon | 0.15 - 0.4 % Show Material materials with Silicon of 0.15 - 0.4 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |