Medium Carbon Steel
ISO 683-1 Grade C45 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Medium Carbon Steel
ISO 683-1 Grade C45 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Medium Carbon Steel
ISO 683-1 Grade C45E quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Acero
ASTM A387 Grade 22 Class 1, Annealed, Normalized and Tempered, or Quenched and TemperedSuministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
ASTM A542 Type A Class 1 Quenched and TemperedSuministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
ASTM A542 Type B Class 1 Quenched and TemperedSuministrada por:
1 proveedor Matmatch
Acero
ASTM A387 Grade 22 Class 1, Annealed, Normalized and Tempered, or Quenched and TemperedSuministrada por:
1 proveedor Matmatch
Acero bajo en carbono
DIN 17200 Grade C22 quenched and tempered (+QT)Acero bajo en carbono
EN 10083-1 Grade C25E quenched and tempered (+QT)Acero bajo en carbono
EN 10083-1 Grade C25R quenched and tempered (+QT)