Description

Materion Brush Performance Alloys’ BrushForm® 96 Strip is a high-performance, heat treatable spinodal copper nickel tin alloy designed to provide optimal formability and strength characteristics in conductive spring applications such as electronic connectors, switches, and sensors. It is available in both pre-heat treated (mill hardened) and heat treatable (age hardenable) forms.

Related Standards

This material data has been provided by Materion Brush GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.91 g/cm³

Show Supplier Material materials with Density of 8.91 g/cm³

Dimension

PropertyValueComment

Thickness

0.04 - 0.5 mm

Show Supplier Material materials with Thickness of 0.04 - 0.5 mm

gauge

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

124 GPa

Show Supplier Material materials with Elastic modulus of 124 GPa

Elongation

23.0 °C

4 %

Show Supplier Material materials with Elongation of 4 %

for strip thicker than 0.10 mm

Hardness, Vickers

23.0 °C

300 - 370 [-]

Show Supplier Material materials with Hardness, Vickers of 300 - 370 [-]

Poisson's ratio

23.0 °C

0.3 [-]

Show Supplier Material materials with Poisson's ratio of 0.3 [-]

Tensile strength

23.0 °C

931 MPa

Show Supplier Material materials with Tensile strength of 931 MPa

Yield strength Rp0.2

23.0 °C

827 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 827 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.62E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.62E-5 1/K

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

5.80E+6 S/m

Show Supplier Material materials with Electrical conductivity of 5.80E+6 S/m

Specific Electrical conductivity

10 % IACS

Show Supplier Material materials with Specific Electrical conductivity of 10 % IACS

Magnetic

PropertyTemperatureValueComment

Relative magnetic permeability

23.0 °C

1.01 [-]

Show Supplier Material materials with Relative magnetic permeability of 1.01 [-]

max.

Chemical properties

PropertyValue

Copper

Balance

Nickel

8.5 - 9.5 %

Show Supplier Material materials with Nickel of 8.5 - 9.5 %

Tin

5.5 - 6.5 %

Show Supplier Material materials with Tin of 5.5 - 6.5 %

Technological properties

Property
Application areas

Electronic connectors, Switches & Sensors