General
Property | Value |
---|---|
Relative density | 8.78 [-] Show Supplier Material materials with Relative density of 8.78 [-] |
Mechanical
Property | Value | Comment |
---|---|---|
Bendability 90°, bw | 0 [-] Show Supplier Material materials with Bendability 90°, bw of 0 [-] | H Temper |
1.5 [-] Show Supplier Material materials with Bendability 90°, bw of 1.5 [-] | EH Temper | |
2 [-] Show Supplier Material materials with Bendability 90°, bw of 2 [-] | SH Temper | |
3.3 [-] Show Supplier Material materials with Bendability 90°, bw of 3.3 [-] | ESH Temper | |
Bendability 90°, gw | 0 [-] Show Supplier Material materials with Bendability 90°, gw of 0 [-] | H Temper |
0 [-] Show Supplier Material materials with Bendability 90°, gw of 0 [-] | EH Temper | |
0.8 [-] Show Supplier Material materials with Bendability 90°, gw of 0.8 [-] | SH Temper | |
1.6 [-] Show Supplier Material materials with Bendability 90°, gw of 1.6 [-] | ESH Temper | |
2.5 [-] Show Supplier Material materials with Bendability 90°, gw of 2.5 [-] | XSH Temper | |
Elastic modulus | 105 GPa Show Supplier Material materials with Elastic modulus of 105 GPa | |
Elongation | 2 % Show Supplier Material materials with Elongation of 2 % | XSH Temper |
2.4 % Show Supplier Material materials with Elongation of 2.4 % | ESH Temper | |
9.2 % Show Supplier Material materials with Elongation of 9.2 % | SH Temper | |
15.3 % Show Supplier Material materials with Elongation of 15.3 % | EH Temper | |
25.6 % Show Supplier Material materials with Elongation of 25.6 % | H Temper | |
Flexural modulus | 100 GPa Show Supplier Material materials with Flexural modulus of 100 GPa | |
Hardness, Vickers | 223 [-] Show Supplier Material materials with Hardness, Vickers of 223 [-] | H Temper |
245 [-] Show Supplier Material materials with Hardness, Vickers of 245 [-] | EH Temper | |
267 [-] Show Supplier Material materials with Hardness, Vickers of 267 [-] | SH Temper | |
285 [-] Show Supplier Material materials with Hardness, Vickers of 285 [-] | ESH Temper | |
305 [-] Show Supplier Material materials with Hardness, Vickers of 305 [-] | XSH Temper | |
Tensile strength | 693 MPa Show Supplier Material materials with Tensile strength of 693 MPa | H Temper |
800 MPa Show Supplier Material materials with Tensile strength of 800 MPa | EH Temper | |
890 MPa Show Supplier Material materials with Tensile strength of 890 MPa | SH Temper | |
1000 MPa Show Supplier Material materials with Tensile strength of 1000 MPa | ESH Temper | |
1058 MPa Show Supplier Material materials with Tensile strength of 1058 MPa | XSH Temper | |
Yield strength | 558 MPa Show Supplier Material materials with Yield strength of 558 MPa | H Temper | for spring material (Kb0.1) |
585 MPa Show Supplier Material materials with Yield strength of 585 MPa | EH Temper | for spring material (Kb0.1) | |
657 MPa Show Supplier Material materials with Yield strength of 657 MPa | H Temper, RP02 | |
661 MPa Show Supplier Material materials with Yield strength of 661 MPa | SH Temper | for spring material (Kb0.1) | |
718 MPa Show Supplier Material materials with Yield strength of 718 MPa | ESH Temper | for spring material (Kb0.1) | |
783 MPa Show Supplier Material materials with Yield strength of 783 MPa | EH Temper, RP02 | |
877 MPa Show Supplier Material materials with Yield strength of 877 MPa | SH Temper, RP02 | |
883 MPa Show Supplier Material materials with Yield strength of 883 MPa | XSH Temper | for spring material (Kb0.1) | |
988 MPa Show Supplier Material materials with Yield strength of 988 MPa | ESH Temper, RP02 | |
1044 MPa Show Supplier Material materials with Yield strength of 1044 MPa | XSH Temper, RP02 |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 1.84e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.84e-05 1/K |
Melting point | 845 - 1000 °C Show Supplier Material materials with Melting point of 845 - 1000 °C |
Specific heat capacity | 375 J/(kg·K) Show Supplier Material materials with Specific heat capacity of 375 J/(kg·K) |
Thermal conductivity | 50 W/(m·K) Show Supplier Material materials with Thermal conductivity of 50 W/(m·K) |
Electrical
Property | Value |
---|---|
Specific Electrical conductivity | 10 % IACS Show Supplier Material materials with Specific Electrical conductivity of 10 % IACS |
Chemical properties
Property | Value | Comment |
---|---|---|
Iron | 0.01 % Show Supplier Material materials with Iron of 0.01 % | max. |
Lead | 0.01 % Show Supplier Material materials with Lead of 0.01 % | max. |
Other | 99.8 % Show Supplier Material materials with Other of 99.8 % | min. | Cu+Sn+P |
Phosphorus | 0.04 - 0.2 % Show Supplier Material materials with Phosphorus of 0.04 - 0.2 % | |
Tin | 9 - 11 % Show Supplier Material materials with Tin of 9 - 11 % | |
Zinc | 0.01 % Show Supplier Material materials with Zinc of 0.01 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | The grade is particularly suitable for electronics (connectors, lead frames, lead terminals, transistor terminals, etc.), electrical (relay and switch contacts, rotary switch slides and contacts, fuse clips, etc.), automotive (bearing frames, hydraulic equipment caps, packing, bearings, clutch disks, electrical parts, etc.) and others (bellows, slides, blades, plate springs, corrosion-proof machinery equipment, diaphragms, etc.) | |
Coating | Standard product specification of a HOT-DIP-tinned strip. *Width means the slit width after plating. *Different plating thickness for each side is possible. * We can accommodate our products to individual specifications other than the above standard specifications. Please feel free to call us. | |
Other | Please contact the supplier if you have any specific requests regarding chemical compostions, mechanical properties, and thickness. | |
Tolerances |