Chromium Molybdenum Steel
EN 10028-2 Grade 12CrMoV12-10 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
ASTM A542 Type E Class 4 Quenched and TemperedSuministrada por:
1 proveedor Matmatch
Acero inoxidable austenítico
ASTM A276 Grade S20910 AnnealedAcero bajo en carbono
EN 10217-3 Grade StE 420 normalized or normalized formed (+N)Acero bajo en carbono
EN 10217-3 Grade StE 460 normalized or normalized formed (+N)Acero bajo en carbono
EN 10217-3 Grade TStE 420 normalized or normalized formed (+N)Acero bajo en carbono
DIN 17125 Grade TStE 420 normalized or normalized formed (+N)Acero bajo en carbono
DIN 17125 Grade StE 420 normalized or normalized formed (+N)Acero bajo en carbono
DIN 17125 Grade StE 460 normalized or normalized formed (+N)Chromium Molybdenum Steel
DIN 17175 Grade 14MoV6-3 quenched and tempered (+QT)Chromium Vanadium Steel
EN 10089 Grade 51CrV4 quenched and tempered (+QT)Unclassified Low Alloy Steel
EN 10217-3 Grade WStE 420 normalized or normalized formed (+N)Unclassified Low Alloy Steel
EN 10217-3 Grade WStE 460 normalized or normalized formed (+N)Unclassified Low Alloy Steel
DIN 17179 Grade WStE 420 normalized or normalized formed (+N)Unclassified Low Alloy Steel
DIN 17179 Grade WStE 460 normalized or normalized formed (+N)Acero inoxidable martensítico
EN 10216-2 Grade X10CrMoVNb9-1 normalized and tempered (+NT)Acero inoxidable endurecido por precipitación
UGI® HT286 Annealed and Cold Drawn and AgedSuministrada por:
Ugitech