Absorción de agua: 6.8 %

Quick Comparison

Polyamide 6 (PA6)

Akulon® K224-HG5

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Zytel® ST811HS NC010

Polyamide 6 (PA6)

Akulon® K222-KGMV14

Suministrada por:

DSM Engineering Materials

Polyamide 66 (PA66)

Zytel® 70K20HSL NC010

Polyamide 66 (PA66)

Zytel® 70K20HSL BK284

Polyamide 6 (PA6)

Akulon® Ultraflow K-FG5

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K224-PG3

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K224-HPG3

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K240-HPG3

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K240-HPG3/A

Suministrada por:

DSM Engineering Materials