Akulon® K240-HPG3/A

Want to keep this datasheet? Save it now in your required format

Description

Akulon® is our family of high performance polyamide 6 and polyamide 66 materials, used by customers across the world in applications ranging from automotive, electronics & electrical, to furniture and packaging.
We offer Akulon® grades for injection molding, blow molding and extrusion (including barrier film, stock shapes, convoluted tubes, and mono and multi filament).
In molded parts the material offers an excellent balance of easy design and processing with outstanding mechanical properties over a wide temperature range and in diverse conditions. Meanwhile for extrusion the strength, resilience and easy processing of Akulon® sets the market standards.

Datasheet URL:

Akulon® K240-HPG3/A

This material data has been provided by DSM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting Standard

Density

1.2 g/cm³

Show Supplier Material materials with Density of 1.2 g/cm³

dry

ISO 1183

Moisture absorption

2 %

Show Supplier Material materials with Moisture absorption of 2 %

dry

Sim. to ISO 62

Water absorption

6.8 %

Show Supplier Material materials with Water absorption of 6.8 %

dry

Sim. to ISO 62

Mechanical

PropertyTemperatureValueConditionTesting Standard

Elastic modulus

3 GPa

Show Supplier Material materials with Elastic modulus of 3 GPa

conditioned

ISO 527-1/-2

5.6 GPa

Show Supplier Material materials with Elastic modulus of 5.6 GPa

dry

ISO 527-1/-2

Elongation

5 %

Show Supplier Material materials with Elongation of 5 %

dry

ISO 527-1/-2

15 %

Show Supplier Material materials with Elongation of 15 %

conditioned

ISO 527-1/-2

Flexural modulus

5 GPa

Show Supplier Material materials with Flexural modulus of 5 GPa

dry

ISO 178

Flexural yield strength

180 MPa

Show Supplier Material materials with Flexural yield strength of 180 MPa

dry

ISO 178

Impact strength, Charpy notched

-30 °C

10 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 10 kJ/m²

dry, conditioned

ISO 179/1eA

23 °C

20 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 20 kJ/m²

dry

ISO 179/1eA

23 °C

30 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 30 kJ/m²

conditioned

ISO 179/1eA

Impact strength, Charpy unnotched

-30 °C

90 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 90 kJ/m²

dry, conditioned

ISO 179/1eU

23 °C

80 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 80 kJ/m²

dry

ISO 179/1eU

Unlock all property charts

Tensile strength

60 MPa

Show Supplier Material materials with Tensile strength of 60 MPa

conditioned

ISO 527-1/-2

110 MPa

Show Supplier Material materials with Tensile strength of 110 MPa

dry

ISO 527-1/-2

Thermal

PropertyValueConditionTesting StandardPressureComment

Heat deflection temperature

185 °C

Show Supplier Material materials with Heat deflection temperature of 185 °C

dry

ISO 75-1/-2

2 MPa

210 °C

Show Supplier Material materials with Heat deflection temperature of 210 °C

dry

ISO 75-1/-2

0.45 MPa

Melting point

220 °C

Show Supplier Material materials with Melting point of 220 °C

dry

ISO 11357-1/-3

10°C/min

Rheological Properties

PropertyTemperatureValueConditionTesting StandardComment

Melt volume-flow rate

275 °C

40 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 40 cm³/10min

dry

ISO 1133

Shrinkage

0.25 %

Show Supplier Material materials with Shrinkage of 0.25 %

dry

ISO 294-4

Parallel

1.2 %

Show Supplier Material materials with Shrinkage of 1.2 %

dry

ISO 294-4

Normal

Technological properties

Property
Fillers

15% Glass Fiber