Mechanical
Property | Temperature | Value |
---|---|---|
Elongation A50 | 20.0 °C | 0 - 17 % Show Material materials with Elongation A50 of 0 - 17 % |
Reduction of area | 20.0 °C | 0 - 35 % Show Material materials with Reduction of area of 0 - 35 % |
Tensile strength | 20.0 °C | 0 - 725 MPa Show Material materials with Tensile strength of 0 - 725 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 0 - 585 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 0 - 585 MPa |
Chemical properties
Property | Value |
---|---|
Boron | 0 - 0.4 % Show Material materials with Boron of 0 - 0.4 % |
Carbon | 0 - 0.3 % Show Material materials with Carbon of 0 - 0.3 % |
Copper | 0 - 0.1 % Show Material materials with Copper of 0 - 0.1 % |
Manganese | 0.8 - 1.1 % Show Material materials with Manganese of 0.8 - 1.1 % |
Molybdenum | 0.2 - 0.3 % Show Material materials with Molybdenum of 0.2 - 0.3 % |
Nickel | 0 - 0.03 % Show Material materials with Nickel of 0 - 0.03 % |
Phosphorus | 0 - 0.04 % Show Material materials with Phosphorus of 0 - 0.04 % |
Silicon | 0 - 0.6 % Show Material materials with Silicon of 0 - 0.6 % |
Sulfur | 0 - 0.035 % Show Material materials with Sulfur of 0 - 0.035 % |