Properties

General

PropertyTemperatureValueComment

Density

20.0 °C

7.8 - 7.9 g/cm³

Show Material materials with Density of 7.8 - 7.9 g/cm³

Typical for Nickel Chromium Molybdenum Steel

Mechanical

PropertyTemperatureValueComment

Elongation A50

20.0 °C

0 - 12 %

Show Material materials with Elongation A50 of 0 - 12 %

Hardness, Brinell

20.0 °C

0 - 311 [-]

Show Material materials with Hardness, Brinell of 0 - 311 [-]

Poisson's ratio

20.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for Nickel Chromium Molybdenum Steel

Tensile strength

20.0 °C

1070 - 1240 MPa

Show Material materials with Tensile strength of 1070 - 1240 MPa

Yield Strength Rp0.2, short transverse

20.0 °C

0 - 930 MPa

Show Material materials with Yield Strength Rp0.2, short transverse of 0 - 930 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

20.0 °C

1.28E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.28E-5 1/K

Typical for Nickel Chromium Molybdenum Steel 20-300°C

Melting point

1529 °C

Show Material materials with Melting point of 1529 °C

Typical for Nickel Chromium Molybdenum Steel

Chemical properties

PropertyValue

Carbon

0.38 - 0.43 %

Show Material materials with Carbon of 0.38 - 0.43 %

Chromium

0.7 - 0.9 %

Show Material materials with Chromium of 0.7 - 0.9 %

Manganese

0.6 - 0.8 %

Show Material materials with Manganese of 0.6 - 0.8 %

Molybdenum

0.2 - 0.3 %

Show Material materials with Molybdenum of 0.2 - 0.3 %

Nickel

1.65 - 2 %

Show Material materials with Nickel of 1.65 - 2 %

Phosphorus

0 - 0.02 %

Show Material materials with Phosphorus of 0 - 0.02 %

Silicon

0.15 - 0.35 %

Show Material materials with Silicon of 0.15 - 0.35 %

Sulfur

0 - 0.01 %

Show Material materials with Sulfur of 0 - 0.01 %