General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Density of 7.8 - 7.9 g/cm³ | Typical for Nickel Molybdenum Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation A50 | 20.0 °C | 0 - 17 % Show Material materials with Elongation A50 of 0 - 17 % | |
Poisson's ratio | 20.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Nickel Molybdenum Steel |
Reduction of area | 20.0 °C | 0 - 35 % Show Material materials with Reduction of area of 0 - 35 % | |
Tensile strength | 20.0 °C | 0 - 725 MPa Show Material materials with Tensile strength of 0 - 725 MPa | |
Yield Strength Rp0.2, short transverse | 20.0 °C | 0 - 585 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 0 - 585 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 20.0 °C | 1.3E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.3E-5 1/K | Typical for Nickel Molybdenum Steel 20-300°C |
Melting point | 1529 °C Show Material materials with Melting point of 1529 °C | Typical for Nickel Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0.05 - 0.2 % Show Material materials with Carbon of 0.05 - 0.2 % |
Copper | 0 - 0.5 % Show Material materials with Copper of 0 - 0.5 % |
Manganese | 0.5 - 0.8 % Show Material materials with Manganese of 0.5 - 0.8 % |
Molybdenum | 0.45 - 0.65 % Show Material materials with Molybdenum of 0.45 - 0.65 % |
Phosphorus | 0 - 0.04 % Show Material materials with Phosphorus of 0 - 0.04 % |
Silicon | 0 - 0.6 % Show Material materials with Silicon of 0 - 0.6 % |
Sulfur | 0 - 0.035 % Show Material materials with Sulfur of 0 - 0.035 % |
Tungsten | 0 - 0.1 % Show Material materials with Tungsten of 0 - 0.1 % |
Vanadium | 0 - 0.03 % Show Material materials with Vanadium of 0 - 0.03 % |