Límite elástico Rp0.5: 221 MPa

Quick Comparison

Cast Copper Brass Yellow Brass

ASTM B584 Grade C86700

Suministrada por:

1 proveedor Matmatch

Wrought Copper Bronze Aluminium Bronze

AMPCO® 8 Rolled sheet and plate

Suministrada por:

AMPCO METAL

Cast Copper Brass Yellow Brass

ASTM B30 Grade C86700

Suministrada por:

1 proveedor Matmatch

Wrought Copper Pure / Low Alloyed Copper

ASTM B301 Grade C14500 H04

Wrought Copper Pure / Low Alloyed Copper

ASTM B301 Grade C14510 H04

Wrought Copper Pure / Low Alloyed Copper

ASTM B301 Grade C14520 H04

Wrought Copper Pure / Low Alloyed Copper

ASTM B301 Grade C14700 H04

Cast Copper Brass Yellow Brass

ASTM B271 Grade C86700 As-Cast

Wrought Copper Bronze Aluminium Bronze

ASTM B150 Grade C61300 HR50

Wrought Copper Bronze Aluminium Bronze

ASTM B150 Grade C61400 HR50

Wrought Copper Bronze Aluminium Bronze

ASTM B150 Grade C61300 HR50

Wrought Copper Bronze Aluminium Bronze

ASTM B150 Grade C62300 HR50

Other Copper Zinc Alloy

ASTM B138 Grade C67500 H02

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95400 Heat-Treated

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95410 Heat-Treated

Wrought Copper High Copper Alloy

ASTM B301 Grade C18700 H04