ASTM B16 Grade C36000 H04 (hard)

.XLSX
.PDF
Save

Description

Related Standards

Properties

Mechanical

Elongation A50 A50

4 - 6 % at 20 °C

Tensile strength Rm

450 - 550 MPa at 20 °C

Yield strength Rp0.5 Rp0.5

205 - 310 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Cu

60 - 63 %

Pb

2.5 - 3 %

Fe

0.35 %

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.