Wrought Copper Pure / Low Alloyed Copper
ASTM B301 Grade C14500 H04Wrought Copper Pure / Low Alloyed Copper
ASTM B301 Grade C14510 H04Wrought Copper Pure / Low Alloyed Copper
ASTM B301 Grade C14520 H04Wrought Copper Pure / Low Alloyed Copper
ASTM B301 Grade C14700 H04Wrought Copper Bronze Aluminium Bronze
ASTM B150 Grade C64210 HR50Wrought Copper Bronze Aluminium Bronze
ASTM B150 Grade C64200 HR50Wrought Copper Bronze Aluminium Bronze
ASTM B150 Grade C61300 HR50Wrought Copper Bronze Aluminium Bronze
ASTM B150 Grade C61400 HR50Wrought Copper Bronze Aluminium Bronze
ASTM B150 Grade C61300 HR50Wrought Copper Bronze Aluminium Bronze
ASTM B150 Grade C62300 HR50Cast Copper Nickel Grade
ASTM B505 Grade C96400Other Copper Zinc Alloy
ASTM B138 Grade C67500 H02Leaded Brass
ASTM B16 Grade C36000 H04 (hard)Tin Brass
ASTM B21 Grade C46200 H04Other Copper Zinc Alloy
ASTM B371 Grade C69400 H04Other Copper Zinc Alloy
ASTM B371 Grade C69430 H04Cast Copper Bronze Aluminium Bronze
ASTM B505 Grade C95800 Heat-TreatedCast Copper Nickel Grade
ASTM B505 Grade C96400Wrought Copper High Copper Alloy
ASTM B301 Grade C18700 H04