EN 10028-3 Grade P460NL1 normalized or normalized formed (+N)

View all suppliers (8)

Want to keep this datasheet? Save it now in your required format

Description

Cryogenic alloy weldable fine grain steel for application in pressure vessel construction.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueConditionRelated StandardsShape

Density

20 °C

7.84 g/cm³

Show Material materials with Density of 7.84 g/cm³

normalized or normalized formed (+N)

EN 10028-3

Sheet, Flat

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

-100 °C

217 GPa

Show Material materials with Elastic modulus of 217 GPa

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

20 °C

210 GPa

Show Material materials with Elastic modulus of 210 GPa

normalized or normalized formed (+N)

EN 10028-3

Flat

20 °C

210 - 212 GPa

Show Material materials with Elastic modulus of 210 - 212 GPa

normalized or normalized formed (+N)

EN 10028-3

Flat

20 °C

212 GPa

Show Material materials with Elastic modulus of 212 GPa

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

100 °C

207 GPa

Show Material materials with Elastic modulus of 207 GPa

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

200 °C

199 GPa

Show Material materials with Elastic modulus of 199 GPa

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

300 °C

192 GPa

Show Material materials with Elastic modulus of 192 GPa

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

400 °C

184 GPa

Show Material materials with Elastic modulus of 184 GPa

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

500 °C

175 GPa

Show Material materials with Elastic modulus of 175 GPa

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

600 °C

164 GPa

Show Material materials with Elastic modulus of 164 GPa

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

Elongation

16.8 %

Show Material materials with Elongation of 16.8 %

Predicted Value, A80

16.9 %

Show Material materials with Elongation of 16.9 %

Predicted Value, A200

18.9 %

Show Material materials with Elongation of 18.9 %

Predicted Value, A80 Transverse

20.5 %

Show Material materials with Elongation of 20.5 %

Predicted Value, A5

22.8 %

Show Material materials with Elongation of 22.8 %

Predicted Value, A50

20 °C

16 %

Show Material materials with Elongation of 16 %

normalized or normalized formed (+N)

EN 10028-3

Sheet, Flat

20 °C

17 %

Show Material materials with Elongation of 17 %

normalized or normalized formed (+N)

EN 10028-3

Flat

20 °C

17 %

Show Material materials with Elongation of 17 %

normalized or normalized formed (+N)

EN 10028-3

Sheet

Transverse

Hardness, Brinell

248 [-]

Show Material materials with Hardness, Brinell of 248 [-]

Predicted Value, Transverse

Poisson's ratio

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Steel

Reduction of area

40.0 %

Show Material materials with Reduction of area of 40.0 %

Predicted Value

44.3 %

Show Material materials with Reduction of area of 44.3 %

Predicted Value, Transverse

Shear modulus

80.2 GPa

Show Material materials with Shear modulus of 80.2 GPa

Predicted Value

Shear strength

526.7 MPa

Show Material materials with Shear strength of 526.7 MPa

Predicted Value

Tensile strength

20 °C

510 - 690 MPa

Show Material materials with Tensile strength of 510 - 690 MPa

normalized or normalized formed (+N)

EN 10028-3

Sheet, Flat

20 °C

510 - 720 MPa

Show Material materials with Tensile strength of 510 - 720 MPa

normalized or normalized formed (+N)

EN 10028-3

Flat

20 °C

510 - 710 MPa

Show Material materials with Tensile strength of 510 - 710 MPa

normalized or normalized formed (+N)

EN 10028-3

Flat

20 °C

520 - 720 MPa

Show Material materials with Tensile strength of 520 - 720 MPa

normalized or normalized formed (+N)

EN 10028-3

Flat

20 °C

520 - 710 MPa

Show Material materials with Tensile strength of 520 - 710 MPa

normalized or normalized formed (+N)

EN 10028-3

Flat

20 °C

520 - 690 MPa

Show Material materials with Tensile strength of 520 - 690 MPa

normalized or normalized formed (+N)

EN 10028-3

Flat

20 °C

540 - 720 MPa

Show Material materials with Tensile strength of 540 - 720 MPa

normalized or normalized formed (+N)

EN 10028-3

Flat

20 °C

540 - 710 MPa

Show Material materials with Tensile strength of 540 - 710 MPa

normalized or normalized formed (+N)

EN 10028-3

Flat

20 °C

540 - 690 MPa

Show Material materials with Tensile strength of 540 - 690 MPa

normalized or normalized formed (+N)

EN 10028-3

Flat

20 °C

570 - 720 MPa

Show Material materials with Tensile strength of 570 - 720 MPa

normalized or normalized formed (+N)

EN 10028-3

Flat

20 °C

570 - 710 MPa

Show Material materials with Tensile strength of 570 - 710 MPa

normalized or normalized formed (+N)

EN 10028-3

Flat

20 °C

570 - 690 MPa

Show Material materials with Tensile strength of 570 - 690 MPa

normalized or normalized formed (+N)

EN 10028-3

Flat

20 °C

630 - 725 MPa

Show Material materials with Tensile strength of 630 - 725 MPa

normalized or normalized formed (+N)

EN 10028-3

Sheet

Transverse

Yield strength

273.8 MPa

Show Material materials with Yield strength of 273.8 MPa

Predicted Value, RP1

318.9 MPa

Show Material materials with Yield strength of 318.9 MPa

Predicted Value, RP1 Transverse

414.3 MPa

Show Material materials with Yield strength of 414.3 MPa

Predicted Value, RP02

475.2 MPa

Show Material materials with Yield strength of 475.2 MPa

Predicted Value, RP02 Transverse

496 MPa

Show Material materials with Yield strength of 496 MPa

Predicted Value, RP002

523.2 MPa

Show Material materials with Yield strength of 523.2 MPa

Predicted Value, RP05

20 °C

370 MPa

Show Material materials with Yield strength of 370 MPa

normalized or normalized formed (+N)

EN 10028-3

Sheet, Flat

20 °C

380 MPa

Show Material materials with Yield strength of 380 MPa

normalized or normalized formed (+N)

EN 10028-3

Flat

20 °C

400 MPa

Show Material materials with Yield strength of 400 MPa

normalized or normalized formed (+N)

EN 10028-3

Flat

20 °C

430 MPa

Show Material materials with Yield strength of 430 MPa

normalized or normalized formed (+N)

EN 10028-3

Flat

20 °C

445 MPa

Show Material materials with Yield strength of 445 MPa

normalized or normalized formed (+N)

EN 10028-3

Flat

20 °C

460 MPa

Show Material materials with Yield strength of 460 MPa

normalized or normalized formed (+N)

EN 10028-3

Flat

20 °C

460 MPa

Show Material materials with Yield strength of 460 MPa

normalized or normalized formed (+N)

EN 10028-3

Sheet

Transverse

Thermal

PropertyTemperatureValueConditionRelated StandardsShape

Coefficient of thermal expansion

-100 °C

1.05e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.05e-05 1/K

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

20 °C

1.15e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.15e-05 1/K

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

100 °C

1.21e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.21e-05 1/K

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

200 °C

1.27e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.27e-05 1/K

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

300 °C

1.32e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.32e-05 1/K

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

400 °C

1.36e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.36e-05 1/K

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

500 °C

1.4e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.4e-05 1/K

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

600 °C

1.44e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.44e-05 1/K

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

Specific heat capacity

-100 °C

423 J/(kg·K)

Show Material materials with Specific heat capacity of 423 J/(kg·K)

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

20 °C

430 J/(kg·K)

Show Material materials with Specific heat capacity of 430 J/(kg·K)

normalized or normalized formed (+N)

EN 10028-3

Flat

20 °C

430 - 461 J/(kg·K)

Show Material materials with Specific heat capacity of 430 - 461 J/(kg·K)

normalized or normalized formed (+N)

EN 10028-3

Flat

20 °C

461 J/(kg·K)

Show Material materials with Specific heat capacity of 461 J/(kg·K)

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

100 °C

479 J/(kg·K)

Show Material materials with Specific heat capacity of 479 J/(kg·K)

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

200 °C

499 J/(kg·K)

Show Material materials with Specific heat capacity of 499 J/(kg·K)

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

300 °C

517 J/(kg·K)

Show Material materials with Specific heat capacity of 517 J/(kg·K)

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

400 °C

536 J/(kg·K)

Show Material materials with Specific heat capacity of 536 J/(kg·K)

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

500 °C

558 J/(kg·K)

Show Material materials with Specific heat capacity of 558 J/(kg·K)

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

600 °C

587 J/(kg·K)

Show Material materials with Specific heat capacity of 587 J/(kg·K)

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

Thermal conductivity

-100 °C

34.7 W/(m·K)

Show Material materials with Thermal conductivity of 34.7 W/(m·K)

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

20 °C

39.7 - 40 W/(m·K)

Show Material materials with Thermal conductivity of 39.7 - 40 W/(m·K)

normalized or normalized formed (+N)

EN 10028-3

Flat

20 °C

39.7 W/(m·K)

Show Material materials with Thermal conductivity of 39.7 W/(m·K)

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

20 °C

40 W/(m·K)

Show Material materials with Thermal conductivity of 40 W/(m·K)

normalized or normalized formed (+N)

EN 10028-3

Flat

100 °C

40.9 W/(m·K)

Show Material materials with Thermal conductivity of 40.9 W/(m·K)

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

200 °C

41 W/(m·K)

Show Material materials with Thermal conductivity of 41 W/(m·K)

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

300 °C

39.9 W/(m·K)

Show Material materials with Thermal conductivity of 39.9 W/(m·K)

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

400 °C

38.2 W/(m·K)

Show Material materials with Thermal conductivity of 38.2 W/(m·K)

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

500 °C

36.1 W/(m·K)

Show Material materials with Thermal conductivity of 36.1 W/(m·K)

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

600 °C

33.8 W/(m·K)

Show Material materials with Thermal conductivity of 33.8 W/(m·K)

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

Thermal diffusivity

-100 °C

11.9 mm²/s

Show Material materials with Thermal diffusivity of 11.9 mm²/s

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

20 °C

11 mm²/s

Show Material materials with Thermal diffusivity of 11 mm²/s

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

100 °C

10.5 mm²/s

Show Material materials with Thermal diffusivity of 10.5 mm²/s

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

200 °C

9.9 mm²/s

Show Material materials with Thermal diffusivity of 9.9 mm²/s

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

300 °C

9.1 mm²/s

Show Material materials with Thermal diffusivity of 9.1 mm²/s

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

400 °C

8.1 mm²/s

Show Material materials with Thermal diffusivity of 8.1 mm²/s

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

500 °C

6.9 mm²/s

Show Material materials with Thermal diffusivity of 6.9 mm²/s

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

600 °C

5.7 mm²/s

Show Material materials with Thermal diffusivity of 5.7 mm²/s

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

Electrical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Electrical conductivity

5 S/m

Show Material materials with Electrical conductivity of 5 S/m

Predicted Value

Electrical resistivity

-100 °C

1.97e-07 Ω·m

Show Material materials with Electrical resistivity of 1.97e-07 Ω·m

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

20 °C

2.6e-07 Ω·m

Show Material materials with Electrical resistivity of 2.6e-07 Ω·m

normalized or normalized formed (+N)

EN 10028-3

Flat

20 °C

2.6e-07 - 2.62e-07 Ω·m

Show Material materials with Electrical resistivity of 2.6e-07 - 2.62e-07 Ω·m

normalized or normalized formed (+N)

EN 10028-3

Flat

20 °C

2.62e-07 Ω·m

Show Material materials with Electrical resistivity of 2.62e-07 Ω·m

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

100 °C

3.13e-07 Ω·m

Show Material materials with Electrical resistivity of 3.13e-07 Ω·m

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

200 °C

3.85e-07 Ω·m

Show Material materials with Electrical resistivity of 3.85e-07 Ω·m

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

300 °C

4.7e-07 Ω·m

Show Material materials with Electrical resistivity of 4.7e-07 Ω·m

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

400 °C

5.69e-07 Ω·m

Show Material materials with Electrical resistivity of 5.69e-07 Ω·m

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

500 °C

6.85e-07 Ω·m

Show Material materials with Electrical resistivity of 6.85e-07 Ω·m

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

600 °C

8.2e-07 Ω·m

Show Material materials with Electrical resistivity of 8.2e-07 Ω·m

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

Chemical properties

PropertyValueConditionRelated StandardsShape

Aluminium

0.005 %

Show Material materials with Aluminium of 0.005 %

normalized or normalized formed (+N)

EN 10028-3

Sheet

0.02 %

Show Material materials with Aluminium of 0.02 %

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

Carbon

0.2 %

Show Material materials with Carbon of 0.2 %

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

Chromium

0.3 %

Show Material materials with Chromium of 0.3 %

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

Copper

0.2 %

Show Material materials with Copper of 0.2 %

normalized or normalized formed (+N)

EN 10028-3

Sheet

0.7 %

Show Material materials with Copper of 0.7 %

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

Manganese

1 - 1.7 %

Show Material materials with Manganese of 1 - 1.7 %

normalized or normalized formed (+N)

EN 10028-3

Sheet

1.1 - 1.7 %

Show Material materials with Manganese of 1.1 - 1.7 %

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

Molybdenum

0.1 %

Show Material materials with Molybdenum of 0.1 %

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

Nickel

0.4 %

Show Material materials with Nickel of 0.4 %

normalized or normalized formed (+N)

EN 10028-3

Sheet

0.8 %

Show Material materials with Nickel of 0.8 %

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

Niobium

0.05 %

Show Material materials with Niobium of 0.05 %

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

Nitrogen

0.025 %

Show Material materials with Nitrogen of 0.025 %

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

Phosphorus

0.025 %

Show Material materials with Phosphorus of 0.025 %

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

0.03 %

Show Material materials with Phosphorus of 0.03 %

normalized or normalized formed (+N)

EN 10028-3

Sheet

Silicon

0.1 - 0.6 %

Show Material materials with Silicon of 0.1 - 0.6 %

normalized or normalized formed (+N)

EN 10028-3

Sheet

0.6 %

Show Material materials with Silicon of 0.6 %

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

Sulfur

0.015 %

Show Material materials with Sulfur of 0.015 %

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

0.02 %

Show Material materials with Sulfur of 0.02 %

normalized or normalized formed (+N)

EN 10028-3

Sheet

Titanium

0.03 %

Show Material materials with Titanium of 0.03 %

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

Vanadium

0.1 - 0.2 %

Show Material materials with Vanadium of 0.1 - 0.2 %

normalized or normalized formed (+N)

EN 10028-3

Sheet

0.2 %

Show Material materials with Vanadium of 0.2 %

normalized or normalized formed (+N)

EN 10028-3

Flat, Sheet

Technological properties

Property
Supplier Disclaimer

The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information.

Do you have a technical question or need more information about this material?

Post it as a comment below and receive answers from engineers and other community members.