Acero inoxidable austenítico
EN 10028-7 Grade X2CrNiMo17-12-2 solution annealed (+AT)Acero inoxidable austenítico
DIN 17440 Grade X2CrNiMo17-12-2 solution annealed (+AT)Acero inoxidable austenítico
DIN 17440 Grade X2CrNiMo17-12-2 quenched (+Q)Acero inoxidable austenítico
EN 10272 Grade X2CrNiMo17-12-2 solution annealed (+AT)Acero inoxidable austenítico
DIN 17456 Grade X2CrNiMo17-12-2 solution heat-treated and quenchedAcero inoxidable austenítico
EN 10028-7 Grade X3CrNiMoBN17-13-3 solution annealed (+AT)Acero inoxidable austenítico
DIN 17440 Grade X2CrNiMo17-13-2 quenched (+Q)Acero inoxidable austenítico
DIN 17440 Grade X2CrNiMo17-13-2 solution heat-treated and quenchedAcero inoxidable austenítico
EN 10312 Grade X2CrNiMo17-12-2 solution heat-treated and quenchedAcero inoxidable austenítico
EN 10216-5 Grade X2CrNiMo17-12-2 solution annealed (+AT)Acero inoxidable austenítico
DIN 17440 Grade X2CrNiMoN17-12-2 quenched (+Q)Acero inoxidable austenítico
EN 10217-7 Grade X2CrNiMo17-12-2 solution annealed (+AT)Acero inoxidable austenítico
EN 10250-4 Grade X2CrNiMo17-12-2 solution annealed (+AT)Acero inoxidable austenítico
EN 10222-5 Grade X2CrNiMo17-12-2 solution annealed (+AT)Acero inoxidable austenítico
DIN 17460 Grade X3CrNiMoN17-13 solution annealed (+AT)Acero inoxidable austenítico
EN 10269 Grade X2CrNiMo17-12-2 solution annealed (+AT)Acero inoxidable austenítico
EN 10269 Grade X2CrNiMo17-12-2 strain-hardened (+C700)Acero inoxidable austenítico
EN 10269 Grade X3CrNiMoBN17-13-3 solution annealed (+AT)Acero inoxidable austenítico
SEW 410 Grade G-X2CrNiMoN18-10 quenched (+Q)Acero inoxidable austenítico
EN 10088-1 Grade X2CrNiMo17-12-2 strain-hardened (+C700)