Acero inoxidable ferrítico
EN 10095 Grade X10CrAlSi18 soft annealed (+A)Acero inoxidable ferrítico
SEW 470 Grade X10CrAlSi18 soft annealed (+A)Acero inoxidable martensítico
DIN 17440 Grade X12CrMoS17 soft annealed (+A)Acero inoxidable martensítico
EN 10088-1 Grade X14CrMoS17 strain-hardened (+C550)Acero inoxidable martensítico
DIN 17440 Grade X12CrMoS17 quenched and tempered (+QT)Acero inoxidable ferrítico
JIS G4312 Grade SUH21 annealed