UGIMA® 4104 QT650

Want to keep this datasheet? Save it now in your required format

Description

UGIMA® 4104 is an improved machinability stainless steel manufactured only by UGITECH.

Its properties are identical to those of UGI 4104, except for its machinability, which is even better:

  • UGIMA® 4104 is a stainless steel produced by the method of inclusion population development and control, UGIMA®, perfected by UGITECH.
  • The new technological advances of UGIMA® 4104 are extremely advantageous, whatever the machining conditions, machine or tooling used.
  • Productivity increases of 4% have been obtained over our UGINE 4104 during turning in the softened condition. Increases of 25% have been obtained in the treated condition and up to 100% when drilling Ø4 mm HSS in the softened condition.

  • Equivalent Materials

    This material data has been provided by Ugitech SA.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValue

    Density

    23.0 °C

    7.9 g/cm³

    Show Supplier Material materials with Density of 7.9 g/cm³

    Mechanical

    PropertyTemperatureValueComment

    Elastic modulus

    20.0 °C

    215 GPa

    Show Supplier Material materials with Elastic modulus of 215 GPa

    100.0 °C

    212 GPa

    Show Supplier Material materials with Elastic modulus of 212 GPa

    200.0 °C

    205 GPa

    Show Supplier Material materials with Elastic modulus of 205 GPa

    300.0 °C

    200 GPa

    Show Supplier Material materials with Elastic modulus of 200 GPa

    400.0 °C

    190 GPa

    Show Supplier Material materials with Elastic modulus of 190 GPa

    Elongation

    23.0 °C

    12 %

    Show Supplier Material materials with Elongation of 12 %

    min.

    Reduction of area

    23.0 °C

    35 %

    Show Supplier Material materials with Reduction of area of 35 %

    min.

    Tensile strength

    23.0 °C

    650 - 800 MPa

    Show Supplier Material materials with Tensile strength of 650 - 800 MPa

    Yield strength Rp0.2

    23.0 °C

    500 MPa

    Show Supplier Material materials with Yield strength Rp0.2 of 500 MPa

    min.

    Thermal

    PropertyTemperatureValueComment

    Coefficient of thermal expansion

    100.0 °C

    1.05E-5 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 1.05E-5 1/K

    for 20 to mentioned temperature

    200.0 °C

    1.05E-5 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 1.05E-5 1/K

    for 20 to mentioned temperature

    300.0 °C

    1.05E-5 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 1.05E-5 1/K

    for 20 to mentioned temperature

    400.0 °C

    1.05E-5 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 1.05E-5 1/K

    for 20 to mentioned temperature

    Unlock all property charts

    Specific heat capacity

    23.0 °C

    460 J/(kg·K)

    Show Supplier Material materials with Specific heat capacity of 460 J/(kg·K)

    Thermal conductivity

    23.0 °C

    25 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 25 W/(m·K)

    Electrical

    PropertyTemperatureValue

    Electrical resistivity

    23.0 °C

    7.3E-7 Ω·m

    Show Supplier Material materials with Electrical resistivity of 7.3E-7 Ω·m

    Magnetic

    PropertyTemperatureValue

    Saturation polarization

    23.0 °C

    1.6 T

    Show Supplier Material materials with Saturation polarization of 1.6 T

    Chemical properties

    PropertyValueComment

    Carbon

    0.1 - 0.15 %

    Show Supplier Material materials with Carbon of 0.1 - 0.15 %

    Chromium

    15.5 - 17.5 %

    Show Supplier Material materials with Chromium of 15.5 - 17.5 %

    Iron

    Balance

    Manganese

    1 - 1.5 %

    Show Supplier Material materials with Manganese of 1 - 1.5 %

    Molybdenum

    0.2 - 0.5 %

    Show Supplier Material materials with Molybdenum of 0.2 - 0.5 %

    Nickel

    0.5 %

    Show Supplier Material materials with Nickel of 0.5 %

    max.

    Phosphorus

    0.04 %

    Show Supplier Material materials with Phosphorus of 0.04 %

    max.

    Silicon

    0.7 %

    Show Supplier Material materials with Silicon of 0.7 %

    max.

    Sulfur

    0.25 - 0.35 %

    Show Supplier Material materials with Sulfur of 0.25 - 0.35 %

    Technological properties

    Property
    Application areas

  • General component manuafacture and screw machining industries
  • Automotive industry
  • Transport industry
  • Electrical appliance industry…

  • Corrosion properties

    EnvironmentBehaviour or use
    Nitric acidUse with caution
    Phosphoric acidPoor
    Sulphuric acidPoor
    Acetic acidUse with caution
    Sodium carbonateUse with caution
    NaCl (Saline mist)Use with caution
    HumidityGOOD
    Sea waterPoor
    OilPoor


    UGIMA® 4104 has excellent ability to withstand corrosion in certain environments. Its corrosion resistance is typical of ferritic stainless steel and is similar to that of 4104 in every respect; its corrosion resistance is similar to that of a 430 ferritic stainless steel, but it is impaired by the high sulphur content in environments liable to cause pitting or crevice corrosion.

    contact the supplier for these types of environments

    This grade is appropriate for all office equipment applications.

    The use of UGIMA® 4104 is compatible with all the fluids, lubricants, oils and greases used in the machining industry.

    However, UGIMA® 4104 is not recommended for use in marine environments and highly oxidising chemical environments.

    Optimum corrosion resistance is obtained where a surface is free from all traces of machining oil or foreign particles (of iron for example).

    UGIMA® 4104 is pickled in the same way as 4104 ferritic steel. This also applies to decontamination.

    Note: the corrosion resistance of a stainless steel depends on many factors related to the composition of the corrosive atmosphere (chloride concentration, presence or absence of oxidizing agents, temperature, pH, agitation or no agitation, and so on), as well as to the preparation of the material (surfaces free from metal particles, surface finish such as hardening, polishing, and so on). Precautionary measures should also be taken for certain tests such as the saline mist test (French standard NFX 41002): for example marking labels that might cause corrosion run-outs and reduce the test resistance time should not be used on the sample.

    General machinability

    The performance of UGIMA® 4104 in machining is exceptionally good, due to the optimisation of the inclusion population. This is true not only for very high speeds and severe cutting conditions, as a result of the UGIMA®, process, but also for low speeds and less severe cutting conditions, because of the new improvements achieved through this latest development. UGIMA® 4104 is therefore particularly appropriate for screw machining, as its improved machinability is effective through an extensive range of cutting conditions and machining operations. Its performance is based on extremely good chip breakability, extended tool life and excellent surface finish.


    ,

    The cutting conditions shown in the tables below are those which we established in the trial phase of the development of UGIMA® 4104.

    If you would like to use the grade to best advantage for your components and working environment, contact our Technical Service.

    Heat Treatment

    UGIMA® 4104 has a soft ferritic structure after being treated up to approximately 830°C. Above this temperature, it forms austenite, which is transformed into martensite by cooling: approximately 50% martensite maximum after treatment to about 1100°C.


  • It can be softened to a ferritic structure at about 780-820°C (minimum 2 hours)
  • It can be hardened to a ferrite + martensite structure between 900°C and 1070°C.
  • +QT650 tempered steel is hardened between 950° and 1070°C and tempered between 550°C and 650°C

  • Hot forming

    Forging: UGIMA® 4104 can be forged.

    It has a low flow stress (hot hardness) similar to that of a type 1.4016 (430) ferritic stainless steel, i.e. approximately 50% of that of type 1.4301 (304) austenitic stainless steel. Heating: between 1100°C and 1250°C; minimum forging temperature: 950°C


    After forging: two-phase ferrite + martensite structure, to be softened, if required.

    Other

    Available products:


    ProductsFormFinitionTolerance
    Hot rolled descled Bars13
    Cold finished drawn, turned, ground Bars6 to 11
    Drawn BarsHexagonal11

    Welding

    This grade is difficult to weld.

    As with all semi-ferritic grades, there are various risks in welding UGIMA® 4104 if certain precautionary measures are not taken (hydrogen induced cold weld cracking, lack of weld ductility, intergranular corrosion, etc.). This operation should therefore be particularly rigorous.

    To minimise the risks of cold weld cracking in a heat-affected zone [and in a weld metal zone, in the event of homogenous welding or welding without filler material], the parts should be preheated to between 150 and 230°C to remove the hydrogen present in the base metal and minimise tensile stress on cooling. If coated electrodes are used, they should be thoroughly dried to ensure that no hydrogen is supplied in the form of water vapour. For the same reasons, in arc welding, the shielding gas must not contain H₂.

    After welding, to restore the resilience of the heat-affected zones [and the weld metal zones, in the event of homogenous welding or welding without filler material], the martensite should undergo a post weld annealing heat treatment at 760°C (1 hour) + quenching to transform it into ferrite + carbides. If there is a risk of the welded components being distorted during hardening, they must be cooled slowly in an oven to 600°C before mandatory quenching to avoid any risk of embrittlement at T < 500°C. To ensure improved weld bead resilience during arc welding, the shielding gas must not contain N₂ and CO₂ is not recommended. In general, the only shielding gas recommended is argon (plus 2% of oxygen for MIG welding only).

    Finally, it is difficult to prevent intergranular corrosion in a heat-affected zone [and in a weld metal zone, in the event of homogenous welding or welding without filler material] and the risk is even greater when high welding energy is used. The welding energy should therefore be minimised to reduce grain boundary chrome depletion by Cr23C6 precipitation.

    If filler metal is required, a homogeneous ferritic filler (430L, or 430LNb for welding thicknesses < 3 mm), or an austenitic filler (ER308LSi, 309LSi, etc.), or a duplex filler (ER312) can be used. The austenitic and duplex filler metals eliminate the risks of cold weld cracking and intergranular corrosion in a weld metal zone, but not in a heat-affected zone. Preheating and post welding heat treatment are therefore required in all cases. Due to the large amount of S in UGIMA® 4104, it is not advisable to use an "Ni base" filler wire, as is sometimes recommended for welding AISI430 semi-ferritic grades (risk of thermal cracking).