Stainless Steel 430F

Want to keep this datasheet? Save it now in your required format

Description

Martensitic stainless steel with very good machining properties due to its sulphur content. However, due to the addition of sulphur, it is unsuitable for welding.

Equivalent Materials

This material data has been provided by Salomons Metalen.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueTemperatureComment

Density

7.8 g/cm³

Show Supplier Material materials with Density of 7.8 g/cm³ at 23.0 °C

23.0 °C

typical for steels

Mechanical

PropertyValueTemperatureComment

Elastic modulus

200 - 210 GPa

Show Supplier Material materials with Elastic modulus of 200 - 210 GPa at 23.0 °C

23.0 °C

typical for steels

Elongation A5

10 - 12 %

Show Supplier Material materials with Elongation A5 of 10 - 12 % at 23.0 °C

23.0 °C

Hardness, Brinell

220 [-]

Show Supplier Material materials with Hardness, Brinell of 220 [-] at 23.0 °C

23.0 °C

Tensile strength

650 - 850 MPa

Show Supplier Material materials with Tensile strength of 650 - 850 MPa at 23.0 °C

23.0 °C

Yield strength Rp0.2

500 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 500 MPa at 23.0 °C

23.0 °C

Chemical properties

Property

Carbon

0.17 %

Chromium

15.5 - 17.5 %

Manganese

1.5 %

max.

Molybdenum

0.2 - 0.6 %

Silicon

1 %

max.

Sulfur

0.15 - 0.35 %