Unclassified Low Alloy Steel
EN 10028-3 Grade P460NL1 normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10028-3 Grade P460NL2 normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Acero bajo en carbono
EN 10217-3 Grade P460N normalized or normalized formed (+N)Acero bajo en carbono
EN 10028-3 Grade P460N normalized and stress-relievedUnclassified Low Alloy Steel
EN 10217-3 Grade P460NL1 normalized or normalized formed (+N)