Acero inoxidable austenítico
EN 10028-7 Grade X2CrNi19-11 solution annealed (+AT)Acero inoxidable austenítico
DIN 17440 Grade X2CrNi19-11 solution heat-treated and quenchedAcero inoxidable austenítico
DIN 17440 Grade X2CrNi19-11 quenched (+Q)Acero inoxidable austenítico
EN 10272 Grade X2CrNi19-11 solution annealed (+AT)Acero inoxidable austenítico
EN 10216-5 Grade X2CrNi19-11 solution annealed (+AT)Acero inoxidable austenítico
DIN 1654-5 Grade X2CrNi19-11 quenched (+Q)Acero inoxidable austenítico
EN 10217-7 Grade X2CrNi19-11 solution annealed (+AT)Acero inoxidable austenítico
EN 10250-4 Grade X2CrNi19-11 solution annealed (+AT)Acero inoxidable austenítico
DIN 1654-5 Grade X2CrNi19-11 cold drawn and quenchedAcero inoxidable austenítico
DIN 1654-5 Grade X2CrNi19-11 cold drawn, quenched and slightly skin passedAcero inoxidable austenítico
DIN 1654-5 Grade X2CrNi19-11 quenched and turnedAcero inoxidable austenítico
EN 10222-5 Grade X2CrNi18-9 solution annealed (+AT)Acero inoxidable austenítico
EN 10088-1 Grade X2CrNi19-11 strain-hardened (+C700)Acero inoxidable austenítico
JIS G4303 Grade SUS304L solution treatedAcero inoxidable austenítico
JIS G4304 Grade SUS304L solution treatedAcero inoxidable austenítico
JIS G4305 Grade SUS304L solution treatedAcero inoxidable austenítico
JIS G3459 Grade SUS304LTPAcero inoxidable austenítico
JIS G3468 Grade SUS304LTPYAcero inoxidable austenítico
JIS G3463 Grade SUS304LTBAcero inoxidable austenítico
JIS G4306 Grade SUS304L hot-rolled and solution annealed