DIN 2.4668

Quick Comparison

Nickel Chromium Iron Alloy

VDM® Alloy 718

Suministrada por:

VDM Metals

Nickel Chromium Iron Alloy

Alloy 718 Nickel Alloy

Nickel Chromium Iron Alloy

VDM® Powder 718 CTP

Suministrada por:

VDM Metals

Nickel Chromium Iron Alloy

Alloy 718 Nickel Alloy (API 6A)

Nickel Chromium Iron Alloy

Alloy 718 / 2.4668

Suministrada por:

Hempel Special Metals

Nickel Chromium Iron Alloy

Nickel 718 Direct Aged

Nickel Chromium Iron Alloy

Nickel 718 As-Fabricated

Nickel Chromium Iron Alloy

Nickel 718 Solution Treated

Nickel Chromium Iron Alloy

Nickel 718 Solution Treated

Nickel Chromium Iron Alloy

Nickel 718 Heat Treated And Aged