Nickel 718 Direct Aged

Want to keep this datasheet? Save it now in your required format

Description

Equivalent Materials

Ashby charts

See where Nickel 718 Direct Aged falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

8.3 g/cm³ at 20 °C

Mechanical

Elastic modulus

E

200 GPa at 20 °C

Show Nickel Chromium Iron Alloy materials with Elastic modulus of 200 GPa at 20 °C

Elongation

A

19 % at 20 °C

Show Nickel Chromium Iron Alloy materials with Elongation of 19 % at 20 °C

Tensile strength

Rm

1530 MPa at 20 °C

Show Nickel Chromium Iron Alloy materials with Tensile strength of 1530 MPa at 20 °C

Yield strength

YS

1330 MPa at 20 °C

Show Nickel Chromium Iron Alloy materials with Yield strength of 1330 MPa at 20 °C

Thermal

Coefficient of thermal expansion

α

1.3E-5 1/K at 20 °C

Melting point

Tm

1260 °C

Specific heat capacity

cp

440 J/(kg·K) at 20 °C

Thermal conductivity

λ

11 W/(m·K) at 20 °C

Electrical

Electrical conductivity

σel

4.23E+8 S/m at 20 °C

Chemical properties

Element

Weight %

Comment

Ni

50 - 55 %

Cr

17 - 21 %

Fe

11.1 - 24.6 %

Nb

4.8 - 5.5 %

Mo

2.8 - 3.3 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.