Superaustenitic Stainless Steel
Sandvik 254 SMOSuministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable austenítico
EN 10088-1 Grade X1CrNiMoCuN20-18-7 solution annealed (+AT)Nickel Chromium Iron Alloy
Sanicro® 35Suministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable austenítico
EN 10028-7 Grade X1CrNiMoCuN20-18-7 solution annealed (+AT)Acero inoxidable austenítico
EN 10216-5 Grade X1CrNiMoCuN20-18-7 solution annealed (+AT)Acero inoxidable austenítico
EN 10217-7 Grade X1CrNiMoCuN20-18-7 solution annealed (+AT)Acero inoxidable austenítico
EN 10250-4 Grade X1CrNiMoCuN20-18-7 solution annealed (+AT)Acero inoxidable austenítico
ASTM A213 Grade S31254 Heat-TreatedAcero inoxidable austenítico
ASTM A193 Grade B8MLCuN Class 1B, Carbide solution treatedAcero inoxidable austenítico
ASTM A193 Grade B8MLCuN Class 1D, Carbide solution treatedAcero inoxidable austenítico
ASTM A193 Grade B8MLCuN Class 2, Carbide solution treated and strain hardened; M20 and underAcero inoxidable austenítico
ASTM A193 Grade B8MLCuNA Class 1A, Carbide solution treated in the finished conditionAcero inoxidable austenítico
ASTM A249 Grade S31254 Heat-TreatedAcero inoxidable austenítico
ASTM A240 Grade S31254 Heat-TreatedAcero inoxidable austenítico
ASTM A182 Grade F44 Solution-AnnealedAcero inoxidable austenítico
ASTM A276 Grade S31254 Annealed; Hot-Finished or Cold-FinishedAcero inoxidable austenítico
ASTM A473 Grade S31254 AnnealedAcero inoxidable austenítico
ASTM A479 Grade S31254 AnnealedAcero inoxidable austenítico
ASTM A988 Grade S31254