ALLOY 1.4547 Plate

Alternative and trade names
ALLOY 1.4547, UNS S31254, 6MO, F44
Want to keep this datasheet? Save it now in your required format

Description

The 6 Mo super austenitic steel combines moderate tensile strength and high ductility with excellent corrosion resistance in seawater and variety of industrial environment.

Related Standards

Equivalent Materials

This material data has been provided by Sverdrup Steel.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Length

2500 - 6000 mm

Show Supplier Material materials with Length of 2500 - 6000 mm

Thickness

1 - 50 mm

Show Supplier Material materials with Thickness of 1 - 50 mm

Width

1250 - 2000 mm

Show Supplier Material materials with Width of 1250 - 2000 mm

Mechanical

PropertyTemperatureValue

Charpy impact energy, V-notch

-46.0 °C

45 J

Show Supplier Material materials with Charpy impact energy, V-notch of 45 J

Elongation

23.0 °C

35 %

Show Supplier Material materials with Elongation of 35 %

Hardness, Brinell

23.0 °C

310 [-]

Show Supplier Material materials with Hardness, Brinell of 310 [-]

Tensile strength

23.0 °C

655 - 850 MPa

Show Supplier Material materials with Tensile strength of 655 - 850 MPa

Yield strength Rp0.2

23.0 °C

310 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 310 MPa

Chemical properties

PropertyValue

Carbon

0.02 %

Show Supplier Material materials with Carbon of 0.02 %

Chromium

19.5 - 20.5 %

Show Supplier Material materials with Chromium of 19.5 - 20.5 %

Copper

0.5 - 1 %

Show Supplier Material materials with Copper of 0.5 - 1 %

Iron

Balance

Manganese

1 %

Show Supplier Material materials with Manganese of 1 %

Molybdenum

6 - 6.5 %

Show Supplier Material materials with Molybdenum of 6 - 6.5 %

Nickel

17.5 - 18.5 %

Show Supplier Material materials with Nickel of 17.5 - 18.5 %

Nitrogen

0.18 - 0.22 %

Show Supplier Material materials with Nitrogen of 0.18 - 0.22 %

Phosphorus

0.03 %

Show Supplier Material materials with Phosphorus of 0.03 %

Silicon

0.8 %

Show Supplier Material materials with Silicon of 0.8 %

Sulfur

0.01 %

Show Supplier Material materials with Sulfur of 0.01 %

Technological properties

Property
Application areas

High resistance to general corrosion. Typical applications: Pumps, valves, chokes, pipework/flanges and manifolds in Oil & Gas Industry.

Corrosion properties

Typically the alloy has PREN of 42-44, which ensure that the resistance to pitting corrosion is high. High resistance crevice corrosion.

Heat Treatment

Solution annealing at min 1150°C followed by water quenching

Welding

Very good