Wrought Copper High Copper Alloy
ASTM B643 Grade C17200 TH04Wrought Copper Brass Yellow Brass
EN 1652 Grade CuZn40 R340Wrought Copper Pure / Low Alloyed Copper
EN 12735-1 Grade Cu-DHP R220Wrought Copper Pure / Low Alloyed Copper
EN 12735-1 Grade Cu-DHP R200Wrought Copper Brass Yellow Brass
EN 12164 Grade CuZn40 R400Wrought Copper Brass Yellow Brass
EN 1652 Grade CuZn40 R400Wrought Copper High Copper Alloy
EN 1652 Grade CuCo2Be THTin Brass
EN 12163 Grade CuZn39Sn1 R340Leaded Brass
EN 12168 Grade CuZn39Pb2 R410Wrought Copper Brass Yellow Brass
EN 12168 Grade CuZn40 O60Wrought Copper Pure / Low Alloyed Copper
EN 1653 Grade Cu-DHP R240Leaded Brass
EN 1652 Grade CuZn39Pb2 R360Wrought Copper Pure / Low Alloyed Copper
EN 12163 Grade Cu-DHP R250Wrought Copper High Copper Alloy
EN 1652 Grade CuBe2 THWrought Copper Bronze Silicon Bronze
EN 1652 Grade CuNi2Si F00Wrought Copper Bronze Silicon Bronze
EN 1652 Grade CuNi2Si THWrought Copper Bronze Silicon Bronze
EN 1652 Grade CuNi2Si TB00Leaded Brass
EN 12163 Grade CuZn35Ni3Mn2AlPb R490Wrought Copper Brass Yellow Brass
EN 1652 Grade CuZn37 O60Tin Brass
EN 12163 Grade CuZn39Sn1 R400