General
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Densidad | 2.69 g/cm³ Show Material materials with Densidad of 2.69 g/cm³ | H22 | EN 573-3, EN 485 | Strip, Sheet, Plate |
2.69 g/cm³ Show Material materials with Densidad of 2.69 g/cm³ | H22 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip |
Medidas
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | ||||
Límite elástico | 80.0 MPa Show Material materials with Límite elástico of 80.0 MPa | H22 | EN 573-3, EN 485 | Strip, Sheet, Plate | RP02 | |
80 MPa Show Material materials with Límite elástico of 80 MPa | H22 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | |||
20.0 °C | 65.0 MPa Show Material materials with Límite elástico of 65.0 MPa | H22 | EN 573-3 | Flat | RP02 Transverse | |
Módulo de cizallamiento | 26.5 GPa Show Material materials with Módulo de cizallamiento of 26.5 GPa | H22 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | ||
Módulo elástico | 69.0 GPa Show Material materials with Módulo elástico of 69.0 GPa | H22 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | H22 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | |||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||||
Resistencia a la tracción | 120.0 - 160.0 MPa Show Material materials with Resistencia a la tracción of 120.0 - 160.0 MPa | H22 | EN 573-3, EN 485, EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Strip, Sheet, Plate, Coil, Sheet, Strip | ||
20.0 °C | 110.0 - 160.0 MPa Show Material materials with Resistencia a la tracción of 110.0 - 160.0 MPa | H22 | EN 573-3 | Flat | Transverse |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 879.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 879.0 - 963.0 J/(kg·K) | Typical for Wrought 5000 Series Aluminium | ||||
Coeficiente de dilatación térmica | 20 °C | 2.38e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.38e-05 1/K | H22 | EN 573-3, EN 485 | Strip, Sheet, Plate | |
100 °C | 2.38e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.38e-05 1/K | H22 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
100 °C | 0.000024 1/K Show Material materials with Coeficiente de dilatación térmica of 0.000024 1/K | H22 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | 20-100°C | |
Conductividad térmica | 138 W/(m·K) Show Material materials with Conductividad térmica of 138 W/(m·K) | H22 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | ||
205 W/(m·K) Show Material materials with Conductividad térmica of 205 W/(m·K) | H22 | EN 573-3, EN 485 | Strip, Sheet, Plate | |||
Temperatura de fusión | 635.0 - 655.0 °C Show Material materials with Temperatura de fusión of 635.0 - 655.0 °C | H22 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
Temperatura máx. de funcionamiento | 150.0 °C Show Material materials with Temperatura máx. de funcionamiento of 150.0 °C | Typical for Wrought 5000 Series Aluminium |
Eléctrico
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Conductividad eléctrica | 31000000.0 S/m Show Material materials with Conductividad eléctrica of 31000000.0 S/m | H22 | EN 573-3, EN 485 | Strip, Sheet, Plate |
Resistividad eléctrica | 3.23e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.23e-08 Ω·m | H22 | EN 573-3, EN 485 | Strip, Sheet, Plate |
4.9e-08 Ω·m Show Material materials with Resistividad eléctrica of 4.9e-08 Ω·m | H22 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % | H22 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
0.1 % Show Material materials with Cobre of 0.1 % | H22 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | |
Galio | 0.03 % Show Material materials with Galio of 0.03 % | H22 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % | H22 | EN 573-3 | Flat |
0.10 % Show Material materials with Hierro of 0.10 % | H22 | EN 573-3, EN 485 | Strip, Sheet, Plate | |
0.1 % Show Material materials with Hierro of 0.1 % | H22 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | |
Magnesio | 0.6 - 1.0 % Show Material materials with Magnesio of 0.6 - 1.0 % | H22 | EN 573-3, EN 485, EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Flat, Strip, Sheet, Plate, Coil, Sheet, Strip |
Manganeso | 0.03 % Show Material materials with Manganeso of 0.03 % | H22 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
0.03 % Show Material materials with Manganeso of 0.03 % | H22 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | |
Otro | 0.05 % Show Material materials with Otro of 0.05 % | H22 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip |
Silicona | 0.08 % Show Material materials with Silicona of 0.08 % | H22 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
0.08 % Show Material materials with Silicona of 0.08 % | H22 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | |
Vanadio | 0.05 % Show Material materials with Vanadio of 0.05 % | H22 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
Zinc | 0.05 % Show Material materials with Zinc of 0.05 % | H22 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
0.05 % Show Material materials with Zinc of 0.05 % | H22 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip |
Technological properties
Property | ||
---|---|---|
Anodizing | Excellent | |
Application areas | Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels; Anodizing quality; Cosmetics: Cosmetics pieces; Automotive trim: Interior trim, Window frame, Marque badges | |
Corrosion properties | Excellent | |
General machinability | Good | |
Welding | Good | |
Workability | Good |