General
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Densidad | 2.72 g/cm³ Show Material materials with Densidad of 2.72 g/cm³ | T78 | EN 573-3, EN 485, EN 755 | Strip, Sheet, Plate, Tube, Bar |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 6000 Series Aluminium | ||||
Dureza Brinell | 105.0 [-] Show Material materials with Dureza Brinell of 105.0 [-] | T78 | EN 573-3, EN 755 | Strip, Sheet, Plate, Tube, Bar | ||
110.0 [-] Show Material materials with Dureza Brinell of 110.0 [-] | T78 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
20.0 °C | 105.0 [-] Show Material materials with Dureza Brinell of 105.0 [-] | T78 | EN 573-3 | Profile, Rod | ||
20.0 °C | 110.0 [-] Show Material materials with Dureza Brinell of 110.0 [-] | T78 | EN 573-3 | Flat | ||
Elongación | 6.0 % Show Material materials with Elongación of 6.0 % | T78 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | A50 | |
8.0 % Show Material materials with Elongación of 8.0 % | T78 | EN 573-3, EN 485, EN 755 | Strip, Sheet, Plate, Tube, Bar | A50 | ||
10.0 % Show Material materials with Elongación of 10.0 % | T78 | EN 573-3, EN 755 | Strip, Sheet, Plate, Tube, Bar | |||
20.0 °C | 6.0 % Show Material materials with Elongación of 6.0 % | T78 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 8.0 % Show Material materials with Elongación of 8.0 % | T78 | EN 573-3 | Profile, Rod | A50 | |
20.0 °C | 8.0 % Show Material materials with Elongación of 8.0 % | T78 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 10.0 % Show Material materials with Elongación of 10.0 % | T78 | EN 573-3 | Profile, Rod | ||
Módulo de cizallamiento | 26.0 - 26.5 GPa Show Material materials with Módulo de cizallamiento of 26.0 - 26.5 GPa | Typical for Wrought 6000 Series Aluminium | ||||
Módulo elástico | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | Typical for Wrought 6000 Series Aluminium | ||||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 6000 Series Aluminium | ||||
Resistencia a la tracción | 340.0 MPa Show Material materials with Resistencia a la tracción of 340.0 MPa | T78 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | ||
360.0 MPa Show Material materials with Resistencia a la tracción of 360.0 MPa | T78 | EN 573-3, EN 755 | Strip, Sheet, Plate, Tube, Bar | |||
20.0 °C | 340.0 MPa Show Material materials with Resistencia a la tracción of 340.0 MPa | T78 | EN 573-3 | Flat | Transverse | |
20.0 °C | 360.0 MPa Show Material materials with Resistencia a la tracción of 360.0 MPa | T78 | EN 573-3 | Profile, Rod | ||
Ángulo de flexión a 90° | 3.0 °/t Show Material materials with Ángulo de flexión a 90° of 3.0 °/t | T78 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | ||
4.0 °/t Show Material materials with Ángulo de flexión a 90° of 4.0 °/t | T78 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
5.0 °/t Show Material materials with Ángulo de flexión a 90° of 5.0 °/t | T78 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
6.5 °/t Show Material materials with Ángulo de flexión a 90° of 6.5 °/t | T78 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 887.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 887.0 - 963.0 J/(kg·K) | Typical for Wrought 6000 Series Aluminium |
Coeficiente de dilatación térmica | 1.6e-05 - 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6e-05 - 2.4e-05 1/K | Typical for Wrought 6000 Series Aluminium |
Conductividad térmica | 170.0 - 220.0 W/(m·K) Show Material materials with Conductividad térmica of 170.0 - 220.0 W/(m·K) | Typical for Wrought 6000 Series Aluminium |
Temperatura de fusión | 555.0 - 655.0 °C Show Material materials with Temperatura de fusión of 555.0 - 655.0 °C | Typical for Wrought 6000 Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 21000000.0 - 34000000.0 S/m Show Material materials with Conductividad eléctrica of 21000000.0 - 34000000.0 S/m | Typical for Wrought 6000 Series Aluminium |
Resistividad eléctrica | 2.9e-08 - 5e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.9e-08 - 5e-08 Ω·m | Typical for Wrought 6000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.5 - 1.1 % Show Material materials with Cobre of 0.5 - 1.1 % | T78 | EN 573-3, EN 485, EN 755 | Profile, Rod, Flat, Strip, Sheet, Plate, Tube, Bar |
Cromo | 0.25 % Show Material materials with Cromo of 0.25 % | T78 | EN 573-3, EN 485, EN 755 | Profile, Rod, Flat, Strip, Sheet, Plate, Tube, Bar |
Hierro | 0.5 % Show Material materials with Hierro of 0.5 % | T78 | EN 573-3 | Profile, Rod, Flat |
0.50 % Show Material materials with Hierro of 0.50 % | T78 | EN 573-3, EN 485, EN 755 | Strip, Sheet, Plate, Tube, Bar | |
Magnesio | 0.6 - 1.2 % Show Material materials with Magnesio of 0.6 - 1.2 % | T78 | EN 573-3, EN 485, EN 755 | Profile, Rod, Flat, Strip, Sheet, Plate, Tube, Bar |
Manganeso | 0.4 - 1.0 % Show Material materials with Manganeso of 0.4 - 1.0 % | T78 | EN 573-3, EN 485, EN 755 | Profile, Rod, Flat, Strip, Sheet, Plate, Tube, Bar |
Silicona | 0.7 - 1.3 % Show Material materials with Silicona of 0.7 - 1.3 % | T78 | EN 573-3, EN 485, EN 755 | Profile, Rod, Flat, Strip, Sheet, Plate, Tube, Bar |
Zinc | 0.1 - 0.7 % Show Material materials with Zinc of 0.1 - 0.7 % | T78 | EN 573-3, EN 485, EN 755 | Profile, Rod, Flat, Strip, Sheet, Plate, Tube, Bar |
Technological properties
Property | ||
---|---|---|
Workability | Excellent workability. |