General
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Densidad | 2.82 g/cm³ Show Material materials with Densidad of 2.82 g/cm³ | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 7000 Series Aluminium | ||||
Dureza Brinell | 20.0 °C | 175.0 - 190.0 [-] Show Material materials with Dureza Brinell of 175.0 - 190.0 [-] | T652 | EN 573-3 | Flat | |
20.0 °C | 175.0 - 185.0 [-] Show Material materials with Dureza Brinell of 175.0 - 185.0 [-] | T652 | EN 573-3 | Flat, Sheet | ||
20.0 °C | 175.0 - 180.0 [-] Show Material materials with Dureza Brinell of 175.0 - 180.0 [-] | T652 | EN 573-3 | Flat, Sheet | ||
20.0 °C | 175.0 [-] Show Material materials with Dureza Brinell of 175.0 [-] | T652 | EN 573-3 | Flat, Sheet | ||
20.0 °C | 180.0 - 190.0 [-] Show Material materials with Dureza Brinell of 180.0 - 190.0 [-] | T652 | EN 573-3 | Flat | ||
20.0 °C | 180.0 - 185.0 [-] Show Material materials with Dureza Brinell of 180.0 - 185.0 [-] | T652 | EN 573-3 | Flat, Sheet | ||
20.0 °C | 180.0 [-] Show Material materials with Dureza Brinell of 180.0 [-] | T652 | EN 573-3 | Flat, Sheet | ||
20.0 °C | 185.0 - 190.0 [-] Show Material materials with Dureza Brinell of 185.0 - 190.0 [-] | T652 | EN 573-3 | Flat | ||
20.0 °C | 185.0 [-] Show Material materials with Dureza Brinell of 185.0 [-] | T652 | EN 573-3 | Flat, Sheet | ||
20.0 °C | 190.0 [-] Show Material materials with Dureza Brinell of 190.0 [-] | T652 | EN 573-3 | Flat | ||
Elongación | 1.0 % Show Material materials with Elongación of 1.0 % | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | A100 | |
2.0 % Show Material materials with Elongación of 2.0 % | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | A100 | ||
4.0 % Show Material materials with Elongación of 4.0 % | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | A100 | ||
5.0 % Show Material materials with Elongación of 5.0 % | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | A100 | ||
6.0 % Show Material materials with Elongación of 6.0 % | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | A100 | ||
20.0 °C | 1.0 % Show Material materials with Elongación of 1.0 % | T652 | EN 573-3 | Flat | Transverse | |
20.0 °C | 1.0 % Show Material materials with Elongación of 1.0 % | T652 | EN 573-3 | Sheet | ||
20.0 °C | 2.0 % Show Material materials with Elongación of 2.0 % | T652 | EN 573-3 | Flat | Transverse | |
20.0 °C | 2.0 % Show Material materials with Elongación of 2.0 % | T652 | EN 573-3 | Sheet | ||
20.0 °C | 4.0 % Show Material materials with Elongación of 4.0 % | T652 | EN 573-3 | Flat | Transverse | |
20.0 °C | 4.0 % Show Material materials with Elongación of 4.0 % | T652 | EN 573-3 | Sheet | ||
20.0 °C | 5.0 % Show Material materials with Elongación of 5.0 % | T652 | EN 573-3 | Flat | Transverse | |
20.0 °C | 5.0 % Show Material materials with Elongación of 5.0 % | T652 | EN 573-3 | Sheet | ||
20.0 °C | 6.0 % Show Material materials with Elongación of 6.0 % | T652 | EN 573-3 | Flat | Transverse | |
20.0 °C | 6.0 % Show Material materials with Elongación of 6.0 % | T652 | EN 573-3 | Flat | ||
Módulo de cizallamiento | 27.1 GPa Show Material materials with Módulo de cizallamiento of 27.1 GPa | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
Módulo elástico | 72.0 GPa Show Material materials with Módulo elástico of 72.0 GPa | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 7000 Series Aluminium | ||||
Resistencia a la tracción | 470.0 MPa Show Material materials with Resistencia a la tracción of 470.0 MPa | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
505.0 MPa Show Material materials with Resistencia a la tracción of 505.0 MPa | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | |||
525.0 MPa Show Material materials with Resistencia a la tracción of 525.0 MPa | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | |||
540.0 MPa Show Material materials with Resistencia a la tracción of 540.0 MPa | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | |||
550.0 MPa Show Material materials with Resistencia a la tracción of 550.0 MPa | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | |||
560.0 MPa Show Material materials with Resistencia a la tracción of 560.0 MPa | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | |||
570.0 MPa Show Material materials with Resistencia a la tracción of 570.0 MPa | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | |||
20.0 °C | 470.0 MPa Show Material materials with Resistencia a la tracción of 470.0 MPa | T652 | EN 573-3 | Flat | Transverse | |
20.0 °C | 470.0 MPa Show Material materials with Resistencia a la tracción of 470.0 MPa | T652 | EN 573-3 | Sheet | ||
20.0 °C | 505.0 MPa Show Material materials with Resistencia a la tracción of 505.0 MPa | T652 | EN 573-3 | Flat | Transverse | |
20.0 °C | 505.0 MPa Show Material materials with Resistencia a la tracción of 505.0 MPa | T652 | EN 573-3 | Sheet | ||
20.0 °C | 525.0 MPa Show Material materials with Resistencia a la tracción of 525.0 MPa | T652 | EN 573-3 | Flat | Transverse | |
20.0 °C | 525.0 MPa Show Material materials with Resistencia a la tracción of 525.0 MPa | T652 | EN 573-3 | Sheet | ||
20.0 °C | 540.0 MPa Show Material materials with Resistencia a la tracción of 540.0 MPa | T652 | EN 573-3 | Flat | Transverse | |
20.0 °C | 540.0 MPa Show Material materials with Resistencia a la tracción of 540.0 MPa | T652 | EN 573-3 | Sheet | ||
20.0 °C | 550.0 MPa Show Material materials with Resistencia a la tracción of 550.0 MPa | T652 | EN 573-3 | Flat | Transverse | |
20.0 °C | 550.0 MPa Show Material materials with Resistencia a la tracción of 550.0 MPa | T652 | EN 573-3 | Sheet | ||
20.0 °C | 560.0 MPa Show Material materials with Resistencia a la tracción of 560.0 MPa | T652 | EN 573-3 | Flat | Transverse | |
20.0 °C | 560.0 MPa Show Material materials with Resistencia a la tracción of 560.0 MPa | T652 | EN 573-3 | Sheet | ||
20.0 °C | 570.0 MPa Show Material materials with Resistencia a la tracción of 570.0 MPa | T652 | EN 573-3 | Flat | Transverse | |
20.0 °C | 570.0 MPa Show Material materials with Resistencia a la tracción of 570.0 MPa | T652 | EN 573-3 | Flat | ||
Ángulo de flexión a 90° | 12.0 °/t Show Material materials with Ángulo de flexión a 90° of 12.0 °/t | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 795.0 - 1050.0 J/(kg·K) Show Material materials with Calor específico of 795.0 - 1050.0 J/(kg·K) | Typical for Wrought 7000 Series Aluminium |
Coeficiente de dilatación térmica | 2.1e-05 - 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.1e-05 - 2.4e-05 1/K | Typical for Wrought 7000 Series Aluminium |
Conductividad térmica | 121.0 - 170.0 W/(m·K) Show Material materials with Conductividad térmica of 121.0 - 170.0 W/(m·K) | Typical for Wrought 7000 Series Aluminium |
Temperatura de fusión | 465.0 - 655.0 °C Show Material materials with Temperatura de fusión of 465.0 - 655.0 °C | Typical for Wrought 7000 Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 18000000.0 - 34000000.0 S/m Show Material materials with Conductividad eléctrica of 18000000.0 - 34000000.0 S/m | Typical for Wrought 7000 Series Aluminium |
Resistividad eléctrica | 2.9e-08 - 5.6e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.9e-08 - 5.6e-08 Ω·m | Typical for Wrought 7000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Circonio | 0.1 - 0.16 % Show Material materials with Circonio of 0.1 - 0.16 % | T652 | EN 573-3, EN 485 | Flat, Sheet, Strip, Plate |
Cobre | 1.5 - 2.0 % Show Material materials with Cobre of 1.5 - 2.0 % | T652 | EN 573-3, EN 485 | Flat, Sheet, Strip, Plate |
Cromo | 0.05 % Show Material materials with Cromo of 0.05 % | T652 | EN 573-3, EN 485 | Flat, Sheet, Strip, Plate |
Hierro | 0.15 % Show Material materials with Hierro of 0.15 % | T652 | EN 573-3 | Flat, Sheet |
0.15 % Show Material materials with Hierro of 0.15 % | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | |
Magnesio | 2.1 - 2.6 % Show Material materials with Magnesio of 2.1 - 2.6 % | T652 | EN 573-3, EN 485 | Flat, Sheet, Strip, Plate |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % | T652 | EN 573-3, EN 485 | Flat, Sheet, Strip, Plate |
Níquel | 0.05 % Show Material materials with Níquel of 0.05 % | T652 | EN 573-3, EN 485 | Flat, Sheet, Strip, Plate |
Silicona | 0.12 % Show Material materials with Silicona of 0.12 % | T652 | EN 573-3, EN 485 | Flat, Sheet, Strip, Plate |
Titanio | 0.06 % Show Material materials with Titanio of 0.06 % | T652 | EN 573-3, EN 485 | Flat, Sheet, Strip, Plate |
Zinc | 5.7 - 6.7 % Show Material materials with Zinc of 5.7 - 6.7 % | T652 | EN 573-3, EN 485 | Flat, Sheet, Strip, Plate |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent |