General
Property | Value | Comment |
---|---|---|
Densidad | 2.65 - 2.7 g/cm³ Show Material materials with Densidad of 2.65 - 2.7 g/cm³ | Typical for Cast 3xx.x Series Aluminium |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Bending Fatigue Strength | 60.0 - 90.0 MPa Show Material materials with Bending Fatigue Strength of 60.0 - 90.0 MPa | F | EN 1706 | Casting | ||
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium | ||||
Dureza Brinell | 80.0 [-] Show Material materials with Dureza Brinell of 80.0 [-] | F | EN 1706 | Casting | ||
20.0 °C | 80.0 [-] Show Material materials with Dureza Brinell of 80.0 [-] | F | EN 1706 | |||
Módulo de cizallamiento | 2.8 GPa Show Material materials with Módulo de cizallamiento of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium | ||||
Módulo elástico | 73.0 - 80.0 GPa Show Material materials with Módulo elástico of 73.0 - 80.0 GPa | Typical for Cast 3xx.x Series Aluminium | ||||
Resistencia a la tracción | 240.0 MPa Show Material materials with Resistencia a la tracción of 240.0 MPa | F | EN 1706 | Casting | ||
20.0 °C | 240.0 MPa Show Material materials with Resistencia a la tracción of 240.0 MPa | F | EN 1706 |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 960.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 960.0 - 963.0 J/(kg·K) | Typical for Cast 3xx.x Series Aluminium | ||||
Coeficiente de dilatación térmica | 20 °C | 1.9999999999999998e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.9999999999999998e-05 1/K | F | EN 1706 | Casting | |
100 °C | 1.9999999999999998e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.9999999999999998e-05 1/K | F | EN 1706 | Casting | ||
100.0 °C | 2e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2e-05 1/K | F | EN 1706 | |||
Conductividad térmica | 20.0 °C | 120.0 - 130.0 W/(m·K) Show Material materials with Conductividad térmica of 120.0 - 130.0 W/(m·K) | F | EN 1706 | Casting | |
Temperatura de fusión | 505.0 - 770.0 °C Show Material materials with Temperatura de fusión of 505.0 - 770.0 °C | Typical for Cast 3xx.x Series Aluminium |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Conductividad eléctrica | 20.0 °C | 14000000.0 - 18000000.0 S/m Show Material materials with Conductividad eléctrica of 14000000.0 - 18000000.0 S/m | F | EN 1706 | Casting |
Resistividad eléctrica | 5.56e-08 - 7.14e-08 Ω·m Show Material materials with Resistividad eléctrica of 5.56e-08 - 7.14e-08 Ω·m | F | EN 1706 | Casting |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 80.25 % Show Material materials with Aluminio of 80.25 % | F | EN 1706 | |
Cobre | 1.5 - 2.5 % Show Material materials with Cobre of 1.5 - 2.5 % | F | EN 1706 | Casting |
Cromo | 0.15 % Show Material materials with Cromo of 0.15 % | F | EN 1706 | Casting |
Estaño | 0.25 % Show Material materials with Estaño of 0.25 % | F | EN 1706 | Casting |
Hierro | 1.1 % Show Material materials with Hierro of 1.1 % | F | EN 1706 | |
1.10 % Show Material materials with Hierro of 1.10 % | F | EN 1706 | Casting | |
Magnesio | 0.3 % Show Material materials with Magnesio of 0.3 % | F | EN 1706 | Casting |
Manganeso | 0.55 % Show Material materials with Manganeso of 0.55 % | F | EN 1706 | Casting |
Níquel | 0.45 % Show Material materials with Níquel of 0.45 % | F | EN 1706 | Casting |
Plomo | 0.25 % Show Material materials with Plomo of 0.25 % | F | EN 1706 | Casting |
Silicona | 10.0 - 12.0 % Show Material materials with Silicona of 10.0 - 12.0 % | F | EN 1706 | Casting |
Titanio | 0.25 % Show Material materials with Titanio of 0.25 % | F | EN 1706 | Casting |
Zinc | 1.7 % Show Material materials with Zinc of 1.7 % | F | EN 1706 | Casting |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: not recommended | |
Corrosion properties | general: not sufficient | |
General machinability | after thermal treatment: acceptable | |
Processing methods | pressure die casting, separately cast test sample |