General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.4 g/cm³ Show Material materials with Densidad of 8.4 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Durchmesser |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 130 [-] Show Material materials with Dureza Brinell of 130 [-] |
Dureza Vickers | 20.0 °C | 135 [-] Show Material materials with Dureza Vickers of 135 [-] |
Elongación | 20.0 °C | 5 % Show Material materials with Elongación of 5 % |
Límite elástico Rp 0,2 | 20.0 °C | 330 MPa Show Material materials with Límite elástico Rp 0,2 of 330 MPa |
Resistencia a la tracción | 20.0 °C | 480 MPa Show Material materials with Resistencia a la tracción of 480 MPa |
Chemical properties
Property | Value |
---|---|
Cobre | 55 - 57 % Show Material materials with Cobre of 55 - 57 % |
Estaño | 0.3 % Show Material materials with Estaño of 0.3 % |
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Otro | Rest Zn, total 0.2 |
Plomo | 1.6 - 3 % Show Material materials with Plomo of 1.6 - 3 % |