General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.3 g/cm³ Show Material materials with Densidad of 8.3 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Durchmesser |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 120 - 150 [-] Show Material materials with Dureza Brinell of 120 - 150 [-] |
Dureza Vickers | 20.0 °C | 125 - 155 [-] Show Material materials with Dureza Vickers of 125 - 155 [-] |
Elongación | 20.0 °C | 18 % Show Material materials with Elongación of 18 % |
Límite elástico Rp 0,2 | 20.0 °C | 210 MPa Show Material materials with Límite elástico Rp 0,2 of 210 MPa |
Módulo elástico | 20.0 °C | 93 GPa Show Material materials with Módulo elástico of 93 GPa |
Resistencia a la tracción | 20.0 °C | 490 MPa Show Material materials with Resistencia a la tracción of 490 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 20.0 °C | 2.11E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.11E-5 1/K |
100.0 °C | 2.11E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.11E-5 1/K | |
Conductividad térmica | 20.0 °C | 80 W/(m·K) Show Material materials with Conductividad térmica of 80 W/(m·K) |
Temperatura de fusión | 860 - 910 °C Show Material materials with Temperatura de fusión of 860 - 910 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 7.80E+6 S/m Show Material materials with Conductividad eléctrica of 7.80E+6 S/m |
Resistividad eléctrica | 20.0 °C | 1.28E-7 Ω·m Show Material materials with Resistividad eléctrica of 1.28E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.3 - 1.3 % Show Material materials with Aluminio of 0.3 - 1.3 % |
Cobre | 59 - 61.5 % Show Material materials with Cobre of 59 - 61.5 % |
Estaño | 0.3 % Show Material materials with Estaño of 0.3 % |
Hierro | 1 % Show Material materials with Hierro of 1 % |
Manganeso | 0.6 - 1.8 % Show Material materials with Manganeso of 0.6 - 1.8 % |
Níquel | 0.6 % Show Material materials with Níquel of 0.6 % |
Otro | Rest Zn, total 0.3 |
Plomo | 1 % Show Material materials with Plomo of 1 % |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |