Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 270 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 270 [-] |
Elongación | 23.0 °C | 25 % Show Supplier Material materials with Elongación of 25 % |
Límite elástico | 23.0 °C | 450 MPa Show Supplier Material materials with Límite elástico of 450 MPa |
Resistencia a la tracción | 23.0 °C | 650 - 880 MPa Show Supplier Material materials with Resistencia a la tracción of 650 - 880 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.02 % Show Supplier Material materials with Azufre of 0.02 % |
Carbono | 0.03 % Show Supplier Material materials with Carbono of 0.03 % |
Cromo | 21 - 23 % Show Supplier Material materials with Cromo of 21 - 23 % |
Fósforo | 0.03 % Show Supplier Material materials with Fósforo of 0.03 % |
Manganeso | 2 % Show Supplier Material materials with Manganeso of 2 % |
Molibdeno | 2.5 - 3.5 % Show Supplier Material materials with Molibdeno of 2.5 - 3.5 % |
Nitrógeno | 0.08 - 0.2 % Show Supplier Material materials with Nitrógeno of 0.08 - 0.2 % |
Níquel | 4.5 - 6.5 % Show Supplier Material materials with Níquel of 4.5 - 6.5 % |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Oil and gas, Marine |