Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 360 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 360 [-] |
Elongación | 23.0 °C | 12 % Show Supplier Material materials with Elongación of 12 % |
Límite elástico | 23.0 °C | 520 - 1000 MPa Show Supplier Material materials with Límite elástico of 520 - 1000 MPa |
Resistencia a la tracción | 23.0 °C | 800 - 1270 MPa Show Supplier Material materials with Resistencia a la tracción of 800 - 1270 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % | |
Carbono | 0.07 % Show Supplier Material materials with Carbono of 0.07 % | |
Cromo | 15 - 17.5 % Show Supplier Material materials with Cromo of 15 - 17.5 % | |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % | |
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % | |
Molibdeno | 0.6 % Show Supplier Material materials with Molibdeno of 0.6 % | |
Níquel | 3 - 5 % Show Supplier Material materials with Níquel of 3 - 5 % | |
Otro | 0.15 - 0.45 % Show Supplier Material materials with Otro of 0.15 - 0.45 % | Nb+Ta |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace, Oil and gas |