Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 215 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 215 [-] |
Elongación | 23.0 °C | 40 % Show Supplier Material materials with Elongación of 40 % |
Límite elástico | 23.0 °C | 200 MPa Show Supplier Material materials with Límite elástico of 200 MPa |
Resistencia a la tracción | 23.0 °C | 500 - 700 MPa Show Supplier Material materials with Resistencia a la tracción of 500 - 700 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % |
Carbono | 0.03 % Show Supplier Material materials with Carbono of 0.03 % |
Cromo | 16.5 - 18.5 % Show Supplier Material materials with Cromo of 16.5 - 18.5 % |
Fósforo | 0.05 % Show Supplier Material materials with Fósforo of 0.05 % |
Manganeso | 2 % Show Supplier Material materials with Manganeso of 2 % |
Molibdeno | 2 - 2.5 % Show Supplier Material materials with Molibdeno of 2 - 2.5 % |
Nitrógeno | 0.11 % Show Supplier Material materials with Nitrógeno of 0.11 % |
Níquel | 10 - 13 % Show Supplier Material materials with Níquel of 10 - 13 % |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Precison components, General Engineering |